Article
Steel’s water reset: Inside the closed‑loop cooling play powering cleaner continuous casting
Water Becomes the New Currency in Continuous Casting: This Is How a Closed‑Loop Design Saves 70–90%
Continuous casting uses a lot of water. However, with closed‑loop cooling and good chemical treatment, make‑up water consumption can fall sharply. Nozzles and strand quality stay protected.
Continuous steel casting (continuous casting of steel) has a reputation for heavy water use. Secondary spray cooling alone can use hundreds of m³ per hour per caster. Many modern plants have already cut raw water use. However, consumption remains several m³ per ton, usually 5–10 m³/ton, according to industry surveys [www.researchgate.net] and [www.researchgate.net].
In China, data show water/steel intensity fell from ~36 m³/ton in 1980 to ~2.5 m³/ton in 2020. The reuse rate rose to ~98% ([www.researchgate.net]). However, at the equipment level, casters still usually spray 50–200 m³/hour or more. One example shows 18 spray nozzles 2 cm in diameter consuming 220 m³/hour of base water.
Water scarcity, cost and outlet wastewater regulations are driving recirculation systems. Closed‑loop cooling can cut make‑up water by 70–90%. The main loss is only evaporation and drift at about 1–10% of the flow. Therefore raw water intake falls sharply ([www.mdpi.com]). Replacing part of the open spray circuit with water‑cooled rollers (dry cooling, cooling without direct spray) has even been shown to cut make‑up by up to half. In one study that is savings of ~1.5 m³/minute (≈50% of the once‑through flow) [www.researchgate.net].
Secondary closed‑loop architecture
Closed-loop secondary cooling collects spray runoff in a sump. The water then goes through a cooling tower or spray pond, is cooled, and goes back to the nozzles. A cooling tower (wet cooling, evaporative cooling with air) takes hot water from the spray pan, cools it by evaporation, then sends it to a surge tank. From there, pumps send the water to the filtration unit and the chemical feeders. Then it goes to the spray header on the caster.
Make-up water is added only to replace the volume that evaporates, usually 3–5% of the circulation, plus blowdown (discharging part of the circulating water to control salt accumulation). The filtration package can consist of filter media and fine-particle polishing. A common option is anthracite sand media such as sand/silica filter media and activated carbon for organics such as activated carbon, followed by cartridge polishing if needed cartridge filter. Chemical dosing is done accurately with a dosing pump.
Cooling tower vs. spray pond
In steel plants, mechanical draft cooling towers are usually the backbone. An induced‑draft tower with fill cools large flows in a compact footprint. Its outlet temperature is close to ~2–3 °C above ambient wet‑bulb, the reference temperature for evaporative cooling. A spray pond is an open basin where warm water is sprayed into the air. It needs much more land and usually only gets down to ~4–10 °C above wet‑bulb, but it has no fans and no fill. Both approaches can share a loop. Primary (mold) cooling is usually already closed‑loop, and the secondary spray loop is added via a shared tank and tower.
Field example: at one plant, all spray water return is filtered and chlorinated. Then it goes to the cooling tower and storage tank before reuse ([www.mdpi.com]). A typical design has a sediment/filter skid to separate particles and oil, chemical injection (scale inhibitor, biocide, corrosion inhibitor, pH adjustment), a surge tank/basin, a pump station to the nozzles, and a twin‑cell cooling tower. Used spray water is collected back in the sump through a drain leg/pan.
Core operating parameters
Engineers choose cycles of concentration to balance blowdown and scaling risk. Cycles of concentration is the ratio of salt concentration in the recirculation to make‑up. An analysis assumed ~100 m³/h evaporation loss in the cooling tower of a 10 MW hot‑strip mill. By holding salts at a chloride target, the loop runs at ~5–6 cycles before blowdown is needed ([www.mdpi.com]). Therefore only ~20% of the recirculation flow is discharged. This saves ~4× make‑up water vs. single‑pass. In general, each increase in cycles raises efficiency. For example, 4 cycles allow ~75% of the water to be reused. A practical target in the tower is 4–8 cycles.
You can recover more water with side‑stream RO/UF. RO is reverse osmosis, a high-pressure membrane. UF is ultrafiltration, a membrane for particles and colloids. One plant in Indonesia treats cooling blowdown and RO reject through a multimedia filter, activated carbon, a softener, and RO. This combination of physical, chemical and membrane processes produces very high-quality recycle water ([jurnalkesehatan.unisla.ac.id]). Managing RO reject is important, because it avoids concentrate discharge. Same link [jurnalkesehatan.unisla.ac.id]. Such an implementation usually uses ultrafiltration pretreatment before brackish‑water RO. For brackish or seawater sources it can even use sea‑water RO, with deionization polishing through EDI when the goal is near‑zero discharge.
Chemical treatment and fouling prevention
In a closed‑loop, scaling and fouling control is key. Without treatment, cooling water quickly deposits [hardness (Ca/Mg carbonate and sulfate salts) and silica](https://beta.co.id/blog/mencegah-kerak-silika-di-boiler-pabrik-sawit-kunci-ada-di-demineralisasi-dan-fosfat) on nozzles, pipes, and steel surfaces. Biological or organic growth and suspended solids can also clog spray orifices. Scale on the steel strand causes [uneven cooling](https://beta.co.id/blog/nozzle-spray-bersih-pendinginan-seragam-panduan-praktis-untuk-continuous-casting) or surface defects. Scale in nozzles reduces flow or even clogs them. Corrosion products (rust) also add particles.
Make-up water usually needs pretreatment. Softening removes Ca and Mg with resin such as ion-exchange resin in a softener unit. Acid injection stops precipitation. Multimedia and carbon filtration remove particles and organics. Inside the loop, an inhibitor and biocide program keeps the quality. The steel industry now uses all-polymer scale and corrosion inhibitors instead of the older phosphate or chromate. Dispersan Cooling Tower Betagard keeps suspended solids and fine crystals dispersed. Blowdown or filtration then carries them away, so they do not stick as soft deposits. In practice, inhibitor dosing runs through a cooling tower chemical package. The package includes scale inhibitors and corrosion inhibitors, plus biocides for biological control.
Halogen use is also common. One plant chlorinates the feed with ~12% NaClO before it enters the tower ([www.mdpi.com]). The regimen can be a periodic on/off oxidizer (chlorine/bromine), or a continuous non-oxidizing biocide. Corrosion inhibitors such as molybdate/nitrite keep the pH at 9–10. This keeps carbon steel passive and prevents iron oxide.
Operational control and instrumentation
Daily operation needs continuous monitoring of conductivity and pH. Blowdown starts at set salinity limits. Coagulation and flocculation can be applied to a side stream to precipitate hardness and further reduce fouling risk. For water clarity, PAC & ACH coagulants neutralize the charge of fine particles, colloids and color so that floc forms that can be settled or filtered. Online instrumentation (turbidity, ORP, halogen sensors) gives tight control and early warning. For program monitoring we provide Monitoring Cooling Tower Sentinel CTS. When the caster is idle, a scheduled “flush cycle” helps clean the nozzles.
Supporting units such as water‑treatment ancillaries keep the operation stable. Membrane systems packages also give an option to expand recycle capacity without changing the main loop.
Empirical results and global benchmarks
A retrofit at a Chinese plant replaced part of the spray bank with water‑cooled rolls. This reduced secondary spray flow by ~48% and cut raw water by ~1.5 m³/min per caster (about half) ([www.researchgate.net]). Globally, best practices such as closed loops, filtration and high cycles have driven water intensity below 3 m³/ton at many plants ([www.researchgate.net], [www.researchgate.net]). In Indonesia, major producers are following the trend. A subsidiary of PT Krakatau Steel is investing in demineralization/desalination to recycle seawater and minimize freshwater intake ([voi.id]).
Poor tower water quality can damage downstream equipment or product (for example, hot‑rolled coil quality) if left untreated ([www.mdpi.com]). A well-maintained closed‑loop can run for months without deposits. One case study shows that a combination of filtration and polymer inhibitors allowed operation at 6–8 cycles of concentration without significant nozzle fouling ([jurnalkesehatan.unisla.ac.id]). The remaining blowdown (usually <10% of the flow) can be sent to the IPAL or treated further. Some plants even recycle blowdown through RO/EDI to approach zero discharge.
Source notes
This analysis summarizes studies and industry reports on water reuse in continuous casting ([www.researchgate.net], [www.researchgate.net]), cooling system design manuals ([www.mdpi.com], [www.mdpi.com]), and technical literature on water treatment ([jurnalkesehatan.unisla.ac.id], [voi.id]).