Article
The steel caster’s water fix: a scale‑pit‑to‑filter train that turns dirty spray into reusable cooling water
Continuous Casting Spray Water: A “scale pit–oil separator–filter” design that turns wastewater into reuse supply
The contaminated flow is small, but the load is heavy. Each strand sends 20–30 m³/h with 5–7 g/L iron scale and ≈30 mg/L oil. Three physical stages do the work: a scale pit, an oil separator and filtration. They give 80–95% reuse and cut the raw-water intake sharply.
Continuous casting (CC, the continuous pouring of molten steel) uses a lot of water. A typical plant uses 250–300 m³ per ton of hot metal (www.mheavytechnology.com). However, more than 90% of that water runs in a closed loop (recirculating cooling) (www.mattech-journal.org).
The problem is the small but heavily contaminated stream from the secondary cooling zone. This is the spray water (cooling water that touches the product), at only about 20–30 m³/h per strand (www.mheavytechnology.com). Iron oxide scale (93% Fe₂O₃) and lubricating oil collect here.
The fix is not complex chemistry. It is mechanical work done in stages: a scale pit (a settling tank for scale), an oil–water separator, and pressure filtration. These three steps bring TSS (Total Suspended Solids) and oil & grease down to reuse levels. Steel plants around the world work this way (trea.com, www.mdpi.com).
Characteristics of continuous casting wastewater
Industry technical sources note that contaminated CC spray water contains 5–7 g/L TSS, and 93% of that is Fe₂O₃ scale. It also contains ≈30 mg/L oil (www.mheavytechnology.com). One strand at 20 m³/h can release ~500–700 kg of solids per hour.
The temperature rise in this stream is usually ~5–7 °C above makeup. In many jurisdictions, including the standards of the Kementerian Lingkungan Hidup (MoEF) Indonesia, post-treatment effluent is expected to be well below TSS 50 mg/L (TSS ≪ 50 mg/L) and oil & grease 5–20 mg/L. These are indicative figures, and they need a multistage train.
In brief, the load per strand for contaminated flow is: flow rate 20 m³/hour (≈480 m³/day), TSS 5,000–7,000 mg/L, oil & grease ~30 mg/L, and ΔT ~5–7 °C (source: www.mheavytechnology.com).
Three-stage treatment train
We propose a compact design: (1) a gravity scale pit to capture coarse scale, (2) an API-type or coalescing oil–water separator for light oil, (3) media filtration for fines and traces of emulsified oil. A vinyl-lined steel scale pit (a vinyl-lined steel tank) acts as the primary settler.
In the oil separation stage, an upflow-type unit or polypropylene coalescer is placed after the scale pit. Surface oil in the pit is removed with a skimmer. A coalescing separator in the oil removal class makes it easier to reach an oil residue in the single-digit mg/L range.
For polishing emulsified oil and small droplets, steel plants usually use the Dissolved Air Flotation (DAF, flotation with dissolved air) option, with flocculant (trea.com). A DAF package can cover this option if the effluent target is stricter.
Scale pit sizing and primary settling
Effective hydraulic loading (flow per area, m³/hour·m²) is about 1.0–1.2 m³/hour·m² (www.mheavytechnology.com). For 20 m³/hour, the tank needs an area of about 17–20 m². With a depth of 3–4 m, the volume is about 50–80 m³ and the residence time is about 2–4 hours.
TSS in the overflow drops sharply, from about 6,000 mg/L to about 300 mg/L (about 95% removal) (www.mheavytechnology.com). A sloped bottom or scraper collects the sludge (iron oxide) for dewatering. In practice, a continuous screw conveyor or filter press can discharge about 2–3 tons of wet sludge/day per strand (about 100–200 kg/hour of solids).
Oil separation and polishing
API/coalescing separators usually run at a residence time of 15–20 minutes (about 5–7 m³ volume) at a flow rate of 20 m³/hour. With a skimmer, more than 90–95% of the oil (from about 30 mg/L) can be removed. This lowers the level to 5 mg/L or less, which is a common target for reuse.
If fine particles need to clump together better, you can add coagulation/flocculation (for example iron salts or polymers) before the secondary clarifier or DAF. Industry studies note that this practice improves purification (www.mdpi.com). You can dose accurately with a dosing pump, using coagulants and flocculants according to how much colloid the water carries.
Pressure media filtration
After the previous stage, the flow passes through the filter media. A duplex pressure filter setup, two parallel units, works well. For example, two filters of ~2 m² each at a flux of 10 m³/m²·hour handle 20 m³/hour and still allow a backwash cycle.
A dual-media sand–anthracite layer is standard in steel process water treatment (www.mdpi.com). For silica sand media, see sand silica. Anthracite is available as anthracite with a 15–20 year lifetime (according to the product description). If dissolved hydrocarbon traces remain, you can add an activated carbon adsorption stage such as activated carbon.
Pressure filter housings for industrial use can be made of pressure-resistant steel, such as steel filter housings up to 150 PSI. This train usually gives turbidity < 10 NTU (Nephelometric Turbidity Unit, a turbidity unit), TSS < 20–30 mg/L, and oil ≲ 2 mg/L. That is enough for reuse.
Performance and mass balance
For 20 m³/hour (~480 m³/day), with an influent of 5–6 g/L solids (≈110 kg/hour), the scale pit captures ~100–110 kg/hour of raw sludge. The overflow is ≈300 mg/L (www.mheavytechnology.com). This means ~6 kg/hour passes downstream. The plant captures ~2,400–2,600 kg of total solids per day (~3 tons). After dewatering with a filter press or a vacuum belt, this becomes ~200–300 kg of dry cake per day.
The oil trap and the filter reduce oil at 20–30 mg/L (≈0.6 kg/hour) by >90%. A residue of 1–2 mg/L means only 20–40 g/hour remains of the 480 m³. This meets common reuse and discharge limits. A final effluent of 5–20 mg/L TSS and < 5 mg/L oil is a realistic result in this configuration.
Reuse potential and closed-loop operation
With that quality, the water goes back to the CC cooling system. In the steel industry, reuse of >80–90% is standard practice (www.mattech-journal.org). The flow is 480 m³/day (20 m³/hour). This volume replaces almost the same amount of makeup.
Global data show an extreme reuse trend. One study reports that a Chinese plant cut raw water consumption per ton from ~36 m³ to ~2.5 m³ by recycling 98% of its water (iwaponline.com). In the CC loop, makeup is needed only to offset evaporation and blowdown. Evaporation loss is usually small, only a few percent of the flow lost as heat.
Dissolved minerals accumulate. Therefore some plants install a small reverse osmosis (RO) unit on condensate or blowdown to desalinate reuse water (www.mdpi.com, www.mdpi.com). That fits the brackish water RO package (maximum TDS 10,000) or the membrane systems platform for industrial water.
In practice, 80–95% of the treated flow can be reused (www.mattech-journal.org). For example, if 20 m³/hour is treated to low oil and solids levels, about 18 m³/hour can be reused. Only about 2 m³/hour of fresh makeup is then needed. At an 80% reuse rate that saves about 384 m³/day, or about 140,000 m³/year per strand. Savings at this scale cut operating costs and water intake directly.
Regulatory compliance and industry practice
Indonesia promotes reuse over disposal. PP No. 22 Tahun 2021 is the umbrella for environmental approval and for water and wastewater quality management (enviliance.com). A physical treatment train can reduce solids by >90% and oil by >90%. The train is gravity settling, skimming or an oil separator, and multimedia filtration. These results are realistic and consistent with industry practice (trea.com, www.mdpi.com).
Key design parameters
Some design anchor figures. The scale pit is about 17–20 m² for 20 m³/hour (loading about 1.0–1.2 m³/hour·m²), depth 3–4 m (volume ≈50–80 m³), retention time about 2–4 hours. An oil separator with a retention time of 15–20 minutes (≈5–7 m³) reduces oil to ≲5 mg/L. DAF is optional for emulsified oil. A duplex sand/anthracite filter (two parallel units, each about 2 m² at 10 m³/m²·hour) reduces residual fines. Activated carbon is optional for trace organics.
Typical output quality is turbidity < 10 NTU, TSS < 20–30 mg/L and oil ≲ 2 mg/L. This is in line with cooling reuse. This train closes the CC loop to ~80–95% reuse and cuts fresh water demand by a similar amount. It also makes it easier to meet the limits usually applied: TSS ≪ 50 mg/L and oil & grease 5–20 mg/L.