WhatsApp

Article

Steel’s thirst is shrinking: inside the closed‑loop cooling play rewriting continuous casting

beta-pramesti-asiaindustry-steel-manufacturingprocess-casting

Closed-loop in Continuous Casting: Water recirculates, heat stays under control, breakout risk falls

Modern steel plants recirculate >90% of cooling water. They limit make‑up to 2–5% and push water intensity to <2 m³/t, even <0.5 m³/t in best practice. The key is a closed circuit with cooling tower/spray pond and strict water treatment, so nozzles stay precise.

Continuous casting burns through large amounts of heat and water in secondary cooling. In modern plants, more than 90% of cooling water is reused. Only a few percent is lost through evaporation and blowdown (partial water discharge to keep salt concentration in check), according to MDPI and ResearchGate. One study recorded an integrated plant with intake ≈28.6 m³/t and discharge 25.3 m³/t, giving net use ~3.3 m³/t (MDPI). EAF (electric-arc furnace) is usually lower at ≈1.6 m³/t because it circulates more water (MDPI).

Those figures are not an exception. NatSteel Singapore reached total water intensity <1.0 m³/t through “high recycling rates” and cascading reuse (ResearchGate). In fact, dry or indirect cooling at the caster can replace almost half of the once‑through spray water (ResearchGate, Everloy). In one case this saved about 1.5 m³/min of raw water (ResearchGate).

The strategy is straightforward. Design all cooling sprays and mold coolers as closed circuits. Cascade from the high-quality circuit (mold) to lower-grade uses before discharge. Then recover almost all blowdown (ResearchGate). At one plant, only ≈1% of the circulation rate is lost to evaporation for a 5 °C drop. Make‑up blowdown averages ≈1% of the flow (ResearchGate). A well-engineered caster circuit usually operates at 5–10 cycles of concentration. Controls such as variable‑speed pumps, flow metering, and automated bleed‑off support this. Globally, worldsteel data shows plant water intensity from <1 to >100 m³/t depending on practice (ResearchGate, MDPI). The trend clearly points to maximum recirculation and minimum discharge (MDPI, ResearchGate).

Caster closed-circuit architecture

The standard scheme works like this. All return water from the spray is collected in a header tank. It is cooled at the heat-rejection stage (cooling tower or spray pond). Then it is pumped back to the spray header. The cooling tower is the most common option. Induced‑draft cells, counterflow or cross‑flow, pass ambient air upward over a falling water film. A small fraction of the water evaporates (∼0.1–0.6% drift plus 1–2% evaporation) (SugarProcessTech).

A well-designed tower cools water to 3–5 °C above the wet-bulb temperature. This is the reference temperature used to assess tower performance. Multi-cell redundancy, high-efficiency fill, drift eliminators and chemical dosing stations are usually installed. Injection is precise with a dosing pump. A compact vertical structure saves land. The footprint is about 1/25 to 1/50 that of an equivalent spray pond (AquaEnergyExpo).

Cooling tower vs spray pond

A spray pond is a shallow basin. Warm water is pumped to low-pressure nozzles ±1–2 m above the surface, and the water releases heat through evaporation and convection as it falls into the pond. However, it needs much more land, usually 20–50× compared with a tower, and it has limited temperature control (outlet temperature depends on ambient conditions) (AquaEnergyExpo, SugarProcessTech). Its advantages are very simple mechanics (no fans) and easy maintenance. At high capacities that need tight control (as well as low drift for indoor installations), forced‑draft towers are usually preferred (AquaEnergyExpo, SugarProcessTech).

Components, sizing, and key metrics

Typical components of a closed caster circuit include: (1) a surge basin/expansion tank for inventory and temperature buffering; (2) circulation pumps for spray pressure, usually ≥10–15 bar, and flow rates from tens to hundreds of m³/h per caster; (3) piping and distribution headers to the cooling-zone nozzles; (4) a cooling tower bank for the heat load, where each 1 °C drop at 100 m³/h is equivalent to ~0.1 MW of heat; (5) instrumentation: flow meters, inlet/outlet temperature sensors, and conductivity or TDS meters; (6) automatic conductivity-based blowdown control; (7) side‑stream solids/grease removal, for example a clarifier, on the warm return line before the tower.

In operation, make‑up water is added to replace evaporation and small leaks. The make‑up can be the plant’s internal treated water or rainwater. Formosa Steel (Taiwan) and JSW Steel (India) report closed water use rates >90% thanks to multi‑tower recirculation (ResearchGate, MDPI).

Water treatment: scaling, corrosion, biofouling

Caster circulation water must be treated. Otherwise scaling (mineral scale), corrosion and biofouling (biological growth) can clog nozzles and insulate the strand/mold surface. Evaporation in the tower raises the concentration of dissolved minerals. Without treatment, calcium carbonate/sulfate will scale on heat exchangers and nozzles. A CaCO₃ deposit only 0.1 mm thick can cut the local heat-transfer coefficient by up to half. That can trigger hot spots or even a breakout (a spill of semi-liquid steel).

In practice, hardness and ionic content are kept moderate. Softening or acid injection can hold calcium <100 mg/L as CaCO₃‑equivalent in the make‑up. A softener unit is usually used to reduce Ca/Mg that causes scale.

Many plants add ion-exchange-based side‑stream demineralization (ion exchange) or reverse osmosis (brackish-water RO) to lower TDS (total dissolved solids) and keep the concentration cycle in the 3–7× range. Phosphonate/polymer-based scale inhibitors (threshold inhibitors) are injected so that reuse can be pushed higher. This formulation is available as a scale inhibitors program for cooling towers.

pH is controlled (usually 7–8 for steel) so that the Langelier Saturation Index is negative. Loop silica is maintained at ~50–100 mg/L with alkalinity <200 mg/L CaCO₃. Closed-loop chemical packages help stabilize pH and protect against corrosion, including amine passivation, as with closed-loop chemicals.

Biofilm control and loop sanitation

Cooling towers are prone to algae, bacteria, and biofilm. Microbial slime on nozzles reduces flow and spray uniformity. Biogenic sulfuric acid corrosion can also occur. Routine doses of biocides (chlorine, bromine, or non‑oxidizing) and UV irradiation are used to suppress growth (biocides, UV system). Make-up water should be low in nutrients and organic load. Some operators do periodic chemical clean‑outs and basin flushing to remove sludge. This service aligns with cooling tower cleaning.

Nozzle and suspended-particle management

Nozzles must be free of particles. Recovered caster water “usually contains foreign matter” that can block spray outlets, reduce cooling uniformity, and cause cracks/defects on the slab surface (Everloy). Therefore a side‑stream filter and pot feeder (safe inline chemical injection points) plus automatic blowdown schedules are standard. For fine-particle polishing, plants usually install a cartridge filter on the bypass. On the coarse line ahead of the pump, a strainer catches debris that can clog nozzles.

For extra safety on mold cooling loops, some plants use deionized make-up or condensate to reduce corrosion. At a minimum, loop pH and dissolved O₂ are kept in range (amine passivation is common in closed cold-water circuits). For permanent deionization, a demineralizer package or EDI (electrodeionization) system gives a mineral-free make-up source.

Impact on water intensity and compliance

With proper maintenance, a caster closed circuit can recycle 95–98% of its water. It then needs only 2–5% make-up. Plant water intensity drops to near the evaporation baseline (~0.1–0.2 m³/t) plus a small bleed. Some plants report a requirement of <0.5 m³ per ton of steel (ResearchGate, MDPI). These steps save water and also reduce the effluent volume. Therefore they help you meet the effluent quality standards for discharge in Indonesia and the international standards.

Source: peer-reviewed studies and industry data (MDPI, ResearchGate, ResearchGate, Everloy). World Steel Association and plant case studies give global water intensity benchmarks from <1 to >100 m³/t. The trend is toward maximum circulation and minimum discharge (MDPI, ResearchGate).