Article
Inside the chemistry race keeping CCGT cooling towers clean — and saving millions of gallons
Inside the chemistry race keeping CCGT cooling towers clean — and saving millions of gallons
A combined-cycle gas turbine's cooling loop is a chemistry problem, and the stakes are measured in megawatts. With a coordinated program of scale and corrosion inhibitors plus a biocide schedule that works, plants are pushing cycles of concentration toward 10× and cutting makeup water by the millions.
Modern combined‑cycle gas turbine (CCGT) plants reject very high heat, tens to hundreds of MWth (thermal megawatts) in the steam condenser, and circulate enormous water volumes. Typical withdrawals run on the order of 7,500–20,000 gallons per MWh of electricity generated (www.ucs.org). As water evaporates in the cooling tower, dissolved minerals concentrate (higher total dissolved solids, TDS). Therefore simple makeup and blowdown cannot prevent scale.
It gets worse as temperature climbs. Even saturated calcium carbonate (CaCO₃) readily precipitates as condenser‑water temperature rises (www.power‑eng.com). And the tiniest fouling matters. About 0.25 mm of biofilm can cut heat transfer by about 50% (irispublishers.com). Also, warm, oxygenated water attacks metals. Mild steel corrosion can exceed 0.2 mm/yr if untreated, and copper‑nickel condenser alloys are also vulnerable.
Cooling towers are fertile grounds for biological growth (algae, bacteria, and Legionella) at 20–50 °C. Therefore they need rigorous microbiological control. The heat load is very high, the cycles of concentration (COC, the ratio of circulating water concentration to makeup water concentration) are high, and the flow rates are large. Therefore the plant needs an aggressive, coordinated chemical regimen, fine‑tuned by precise feed systems such as dosing pumps.
When plants get this right, the savings show on the water meter. In one case, better treatment and polishing of the makeup water let the plant run at about 9.8× cycles instead of 2×. That saved about 1.94×10^6 gallons of makeup water a year (www.prochemtech.com). In another case, cycles went up to 9.85× and saved about 5.0×10^6 gallons a year (about US$70.6k) (www.prochemtech.com).
Scale control chemistry and pH management
The main scales in tower and condenser loops are calcium carbonate, calcium sulfate, calcium phosphate, silica and metal hydroxides. Industry practice pairs chemical inhibitors with controlled blowdown. One simple tactic is acidity control. For example, H₂SO₄ dosing converts bicarbonate alkalinity to CO₂ and H₂O (www.power‑eng.com). The acid must be fed accurately, for example with a dosing pump.
Modern programs use blends of phosphonate and polymer that hold Ca²⁺ and stop CaCO₃ from forming scale above its limit. A typical dose is phosphonates (for example HEDP, ATMP) at about 5–20 mg/L plus polyacrylate and related polymers at 1–5 mg/L. This allows more cycles, usually 2–4× on hard water (www.prochemtech.com). This is the sweet spot for scale inhibitor formulations. Dispersive polymers (for example polyacrylates and silicates) act as dispersants and keep the precipitates stable.
Makeup water quality is the lever. In very hard waters, some plants pre‑soften makeup to <20 mg/L Ca²⁺, which allows ~10× cycles (see metrics below). Pretreatment options range from conventional softeners to hardness‑targeted pressure membranes such as nano‑filtration (qualitatively, NF removes multivalent hardness at lower pressure than RO). In some cases the plant polishes with brackish‑water RO if TDS is the constraint. Where RO is deployed, upstream protection with ultrafiltration helps when makeup is drawn from surface waters.
Historically, plants fed phosphate (ortho‑ or polyphosphate) to precipitate calcium as calcium phosphate (www.power‑eng.com). But phosphates are also nutrients for algae, and environmental regulations now usually restrict them (www.power‑eng.com). In one U.S. plant, eliminating phosphate ended algal blooms. The plant switched to a film‑forming organic starch inhibitor (FlexPro® RPSI) and cut carbon‑steel corrosion from ~0.2–0.25 mm/yr to ~0.0025–0.0075 mm/yr (www.power‑eng.com). That trend is phosphate‑free programs using biodegradable polymers or polycarboxylates (for example polyaspartate, polysilicate blends). Plants use them more and more to control scale with negligible nutrient loading (www.power‑eng.com) (www.researchgate.net).
One example: a plant raised cooling cycles from 2× to ~10×. It used softened makeup and inhibitors that work at high cycles. Bulk Ca hardness fell from ~186 to ~19 mg/L as CaCO₃ (www.prochemtech.com) (www.prochemtech.com). Total alkalinity climbed to ~1,660 mg/L, because most of the calcium was removed, as expected at high cycling. No visible CaCO₃ deposits occurred, even on “blowdown‑limited” heat exchangers. In practice, the water analysis sets the targets. For example, keeping hardness <50 mg/L (as CaCO₃) and silicon <10–30 mg/L keeps carbonate or silica scale well below the levels where it becomes a problem.
Corrosion inhibitor packages by metallurgy
Cooling loops mix carbon steel piping, copper‑nickel condenser tubes, stainless steels, and sometimes galvanized (zinc‑coated) components. A multi‑component inhibitor package is typical. It is delivered as part of a broader cooling tower chemical program.
For carbon steel, running bulk water at a mildly alkaline pH (usually 8.0–9.0) helps keep corrosion low. Orthophosphate or silicate (30–60 mg/L as Na₂SiO₃) forms a protective film. Traditional polyphosphate “passivators” (10–30 mg/L PO₄³⁻) deposit an amorphous Fe/PO₄ layer on the steel (watertechnologyreport.wordpress.com). Newer branched polymers, for example polyacrylates or polysilicates, can form thin barriers that give very low rates (~0.1 mm/yr or less) (www.power‑eng.com). This is the field of modern corrosion inhibitors. In practice, a well‑treated tower can hold mild‑steel corrosion at 0.25–0.5 mils/yr (0.006–0.012 mm/yr) at 10× cycles (www.prochemtech.com).
Copper–nickel tubes need azoles, tolyltriazole or benzotriazole at ~1–5 mg/L. These adsorb onto the copper surface and block attack. A cited program includes tolyltriazole for copper corrosion control (www.prochemtech.com).
Galvanized steel brings a different risk. “White rust” on zinc surfaces can occur above pH ~8.2 (www.prochemtech.com). Modern formulations add a specific “white rust inhibitor” (usually borate‑ or silicate‑based). One program kept 4–12 mg/L of such inhibitor and fully eliminated white rust at pH ~9+ (www.prochemtech.com). Stainless alloys usually passivate by themselves, but keeping chloride low (<200 mg/L) avoids pitting.
Performance data from a COC‑10 program showed corrosion coupon rates of mild steel <0.2 mil/yr (0.005 mm/yr) and copper <0.05 mil/yr (www.prochemtech.com). AWT guidance judged this “excellent”. Another example gave copper corrosion ~0.01 mil/yr in a glass‑plant system (www.prochemtech.com).
Biocide schedules and microbial targets
Warm, oxygenated tower water is ideal for [microbial growth, including Legionella](https://beta.co.id/en/blog/inside-the-highstakes-war-on-legionella-in-powerplant-cooling-towers). Programs combine oxidizing biocides (chlorine, bromine, chlorine dioxide) with periodic non‑oxidizing agents. These are fed through controlled feed equipment and, where appropriate, on‑site oxidant generation such as electrochlorination. A curated portfolio of biocides underpins the regimen.
Oxidizing biocides usually run on a combined continuous and slug plan. A low continuous dose (for example about 0.2–0.5 mg/L Cl₂ or Br₂) keeps background control. Periodic "shock" treatments (for example 2–5 mg/L for 10–60 minutes) break up established biofilms (irispublishers.com). Chlorine dioxide (ClO₂) still works at high pH. It makes no THMs and does not react with ammonia or inhibitors. It is usually dosed at about 0.5–1.0 mg/L as a continuous dose or a short feed, with boosts to 1–3 mg/L from time to time (irispublishers.com).
Non‑oxidizing biocides tackle chlorine‑resistant strains and entrenched slimes. Aldehydes (for example glutaraldehyde) or organic bromides (DBNPA, THPS) are dosed 5–25 mg/L for short contacts (1–4 h) once per week or month. Glutaraldehyde (50% active) is usually fed at 15–25 ppm (as active) for 2–4 h weekly. Algaecide combinations (for example magnesium or zinc bromides/nitrates) and periodic polyquat shocks can help. Many programs alternate halogen oxidizers and non‑oxidizers to prevent resistance.
One field example: at the Kamojang power plant (Indonesia), injecting 2 ppm NaOCl into the cooling water dropped bacterial counts from ~19,000 to ~100 CFU/mL and raised cooling efficiency ~17.4% (www.researchgate.net). Targets after treatment usually include <10³ CFU/mL total heterotrophic bacteria (CFU, colony‑forming units, heterotrophic plate count) and undetectable Legionella (while no universal limit exists, many guidelines use <100 CFU/100 mL for potable systems). Regular ATP or HPC testing, plus on‑line ORP or UV254 monitors, confirm biocide effectiveness.
Cycles, setpoints, and verification data
Blowdown controls COC. It holds conductivity and TDS at a setpoint that balances water saving against fouling risk. Plants usually target about 5–10× cycles on moderate TDS. Extreme cases with softened makeup can reach 10–15×. One program held COC at about 9.8 at pH 9.4 (www.prochemtech.com), so blowdown dropped a lot. Pretreatment that supports higher cycles includes selective polishing and makeup conditioning with systems like softeners or RO. The supporting equipment (valving, control, tanks) comes from water treatment ancillaries.
Indicative water quality limits under treatment include Ca²⁺ <20–50 mg/L, silica <30–50 mg/L (as reactive silica), alkalinity <1,500 mg/L, and pH 8.5–9.5. Regular lab tests confirm scale indices near zero, for example the “Pendans” or Langelier index ≤–2. Corrosion verification depends on coupons or probes. The targets are <0.1 mm/yr (4 mils/yr) for mild steel and <0.01–0.02 mm/yr (0.4–0.8 mils/yr) for copper alloys. The successful cases above achieved <0.2 mil/yr for steel and <0.05 mil/yr for copper (www.prochemtech.com).
We track scale and fouling with periodic tube inspections and heat-transfer "approach" measurements. The goal is negligible scale on condenser tubes and drift eliminators. With good chemistry, [condensers stay clean enough](https://beta.co.id/en/blog/inside-the-chemistry-race-keeping-power-plant-condensers-clean-and-megawatts-on-line) to keep the design pressure drop and heat transfer. Over time, plants measure the gains: fewer unplanned cleanings, a steadier temperature rise, and less blowdown. In the cited examples, aggressive programs gave a 54–80% reduction in makeup/blowdown and a 17–18% increase in tower heat rejection efficiency (www.prochemtech.com) (www.researchgate.net).
Compliance, discharge, and environmental choices
Modern programs aim to minimize discharges that harm the environment. Phosphorus-free chemistries protect downstream ecosystems (eutrophication concerns) (www.power‑eng.com). Biocide residuals are neutralized (for example, bisulfite added to blowdown to quench chlorine) to meet limits on halogen or biocide in effluent. Corrosion inhibitors are selected without chromium or heavy metals under stringent standards. In Indonesia, for example, power plants must comply with wastewater standards (for example, Permen-LH) that effectively constrain heavy metals and nutrients from cooling tower blowdown.
What a coordinated program looks like
A good CCGT cooling water program combines exact chemical dosing with active monitoring. We feed a strong inhibitor blend continuously to prevent scale and corrosion. The blend is usually phosphonates, polymers, silicates and azoles. It is supported by targeted products such as scale inhibitors and corrosion inhibitors. A mixed biocide schedule (oxidizing + non-oxidizing) stops bio-growth. Controlled feeds and instruments guide it. Where needed, makeup conditioning with nano-filtration or softening raises the cycles we can reach. Routine services keep the system clean, together with a cooling tower chemical program.
The outcomes can be measured. COC is higher, usually double or triple the effective cycling. Condenser fouling stays low, with more than 90% of design heat transfer maintained. Corrosion rates are about 0.01–0.02 mm/yr on steel and copper (www.power‑eng.com) (www.prochemtech.com). These data guide the blowdown setpoints and the chemical feeds. Those are the operational levers that protect plant efficiency and lifespan.
Sources: We used authoritative industry literature and case studies for the data and guidelines (www.power‑eng.com) (irispublishers.com) (irispublishers.com) (www.power‑eng.com) (www.prochemtech.com) (www.prochemtech.com) (www.researchgate.net).