Article
The steel mill that drinks its own water: inside the API‑DAF‑filter loop turning oily scale into supply
Scale Pit–API–DAF: A Wastewater Design for Steel Rolling Mills That Recovers 80–90% of the Water
Mill scale and oil loads can be handled with a three-stage chain: scale pit, oil separator, and filtration. This gives clear water for cooling and reuse above 80%, in line with “quality standards”.
Hot/cold rolling mills generate heavy wastewater: mill scale (iron oxide) and oil/grease from coolant and lubrication. Even so, modern steel mills recycle a large share of their water. A study by Colla et al. shows an integrated mill withdraws ≈28.6 m³/ton and discharges 25.3 m³/ton. Net consumption is only ≈3.3 m³/ton (www.mdpi.com). In practice, about 88–94% of incoming water is recycled (www.mdpi.com). A survey of steel mills in China confirms high reuse: 25 of 31 (~81%) exceeded 70% reuse, and about 32% exceeded 90% (iwaponline.com).
In Indonesia, the Krakatau Posco facility treats 17,000 m³/day of process water, including rolling effluent. It reuses about 700 m³/day (lestari.kompas.com). This refers to national quality standards for discharge to sea or reuse (lestari.kompas.com). At the facility, raw water is treated for steelmaking. After full reverse osmosis (RO) the conductivity is below 80 µS (lestari.kompas.com).
Waste composition and water balance
Rolling wastewater is mostly mill scale (iron oxide) and oil/grease, plus trace metals. The end target is water recovery well above 80%. For context, an electric arc furnace (EAF) can even reach ≈1.6 m³/ton net consumption (www.mdpi.com).
Scale pit and heavy solids settling
The first gate is the scale pit, a deep sedimentation basin for settling mill scale and sand. Typical retention time is ~30–60 minutes (nepis.epa.gov) so that 50–100 μm particles settle. A common design is an elongated rectangular basin (length:width ratio ≥5:1) with a depth of ~8–10 m or more, equipped with a surface oil skimmer and a bottom sludge pump. Heavy sludge is dredged periodically, for example weekly with a grab/clamshell, and is usually recycled to the sinter plant.
Field data support this approach. A US EPA study showed that a trio of scale pits at a hot strip mill captured ≈4,085 tons of iron scale in 11 months (≈124 t/day). That is equivalent to ~1,300 mg/L TSS (total suspended solids) in the influent (nepis.epa.gov). Therefore the pit effluent reported “low net quantities of TSS”, and practically almost all iron oxide was captured (nepis.epa.gov). Important note: this pit does not reduce oil/grease levels. The same study noted no effect on oil/grease (nepis.epa.gov).
API oil separation and DAF flotation
Once the scale is removed, the next targets are oil and light particles. A standard sequence combines an API gravity separator (American Petroleum Institute, a density-based oil-water separator) and DAF (dissolved air flotation). The API separator is a horizontal-flow tank (L:W ≈5:1). It runs at a velocity of <3 ft/min. This floats free oil (free oil, non-emulsified) and settles solids. In typical operation, 80–90% of free oil is skimmed. For this stage, industrial wastewater oil separation covers the units and their chemical program.
The API effluent then enters the DAF. Here, injected air-saturated water forms microbubbles that attach to oil droplets and fine particles, then float them as surface sludge. DAF usually handles oil/TSS loads up to ~500 mg/L and removes ≈95% of oil and TSS. Practical applications usually add coagulant or flocculant before the DAF to enlarge the agglomerates. Accurate chemical feeders such as a dosing pump are needed, together with chemical packages of coagulants and flocculants. Ready-to-use units are available as industrial DAF for FOG and TSS.
This API+DAF combination usually produces oil residue in water in the single-digit mg/L range and removes most of the TSS. From a regulatory standpoint, a TSS of ≈30 mg/L (30-day average) is considered achievable with a clarifier and flotation (nepis.epa.gov). This is in line with the role of clarifier in many industrial schemes.
Multimedia filtration and final polishing
The final stage is tertiary filtration. It removes the remaining fine solids and polishes the water so it is ready for reuse. The usual options are multimedia filters (sand/anthracite), cartridge filters, or membranes when the quality needs to be very high. One plant uses “high‑rate filters” with slag/rock media to reach very low effluent TSS, clear for cooling tower feed (givemechallenge.com). At this stage the media are usually sand silica and anthracite. The filter vessels come as Betaqua Mild Steel Media Filters. A cartridge filter then gives more polishing, and activated carbon is used if trace oil/organics need to come down further.
For extreme recycling, ultrafiltration (UF) or reverse osmosis (RO) can follow. Colla et al. note that coupling UF with RO produces “very high quality” water suitable for reuse (www.mdpi.com). This is where ultrafiltration systems as pretreatment and brackish water RO packages, or the membrane systems platform, are usually placed. The final quality specification still depends on each plant’s process.
Reuse criteria differ by application. For cooling tower make-up, TSS stays at a few mg/L with low turbidity. For very high quality, for example descaling water or utilities, conductivity and hardness are also checked. In practice, the clear filter effluent in the hot-strip mill example is pumped back to the cooling tower for reuse (givemechallenge.com). Reuse water carries residual salts into the cooling circuit. Therefore scale inhibitor cooling tower also affects the reliability of that loop.
Process reuse and plant water balance
With a scale pit → API → DAF → filtration train, treated water usually returns to the plant circuit, mainly as cooling water. Colla et al. describe a hot strip mill where, after sedimentation and decantation, the water “goes to the cooling tower” for reuse (www.mdpi.com). Another field example: polished filter effluent is pumped back to the cooling tower (givemechallenge.com).
In numbers, a reuse target of 80–90% is realistic. The impact is large. For 1 ton of steel, fresh water demand falls from ~28 m³ to ≈3 m³ (www.mdpi.com). In Indonesia, the Krakatau Posco facility confirms this approach. It treats 17,000 m³/day and reuses about 700 m³/day at a quality that meets the standards (lestari.kompas.com, lestari.kompas.com, lestari.kompas.com).
Quality standard compliance and performance indicators
The system above is designed to meet national quality standard limits, for example PermenLHK for TSS and oil. Operational targets are ≤30–50 mg/L TSS and oil close to zero. This is consistent with the US EPA assumption that 30 mg/L TSS can be achieved with a clarifier and flotation (nepis.epa.gov). The Krakatau Posco facility treats to quality standards for both discharge to the sea and reuse (lestari.kompas.com).
In short, a scale pit train + API/DAF + filtration usually removes >95% TSS and oil. The effluent then meets regulations. Reuse usually exceeds 80%, which cuts wastewater volume by ≈90% and fresh water consumption by the same amount. This is in line with circular economy targets (www.mdpi.com, iwaponline.com). Example metrics: one Indian hot strip mill reported polished water at ~2–3 mg/L solids, so it can be recycled (givemechallenge.com). A Chinese project showed UF+RO producing “very high quality” water (conductivity 80 µS) and encouraging reuse rather than discharge (www.mdpi.com, lestari.kompas.com).