Steel’s heat-transfer bottleneck: inside the chemistry that keeps exchangers clean

beta-pramesti-asiaindustry-steel-manufacturingprocess-cooling-water-systems-contact

Cooling Water in a Steel Plant: Online Antifouling and Chemical Cleaning That Keep Heat Exchangers Sharp

Mineral scale and biofilm can cut heat exchanger efficiency within weeks. This guide covers the preventive and chemical cleaning steps steel plants use to hold back fouling and save on shutdown costs.

In a steel plant, recirculating cooling water usually runs through a cooling tower. It carries intense heat from the furnace to the rolling mill. High flow rates and elevated temperatures cause minerals to precipitate and foul the water. Therefore deposits stick to hot surfaces. These deposits include calcium carbonate, sulfate, phosphate, silicate, suspended sediment, corrosion oxides (iron oxyhydroxides), and biofilm.

For example, CaCO₃ and CaSO₄ have "inverse solubility" with temperature. The hotter it gets, the more readily they deposit. They form an insulating layer and raise pressure drop. Therefore pumps work harder for the same cooling duty. Without control, fouling causes unplanned shutdowns and high cleaning costs.

Deposit profile and thermal penalty

The main foulants in the cooling circuit are mineral scale and biofilm. This holds for non-contact circuits (loop heat exchanger, condenser) and contact circuits (direct quenching, spray cooling). They act directly on the heat transfer coefficient and flow capacity. Industry best practice puts "online prevention" at the front line.

Water quality and side-stream filtration

Circuit design first minimizes incoming particles (filter, clarifier, side-stream polishing) and controls blowdown so total dissolved solids (TDS) stay under control. Many plants choose [raising cycles of concentration](https://beta.co.id/blog/hemat-air-di-menara-pendingin-dorong-coc-setinggi-mungkin-reuse-air-limbah-dan-untungnya-nyata), COC (ratio of dissolved salt concentration in the loop compared with make-up) to save water and blowdown. This is a global trend that includes recycling "gray" water full of impurities.

Key parameters are monitored to keep LSI (Langelier Saturation Index, an index of the tendency for CaCO₃ precipitation) near zero. The water stays slightly undersaturated so it does not trigger scale. These parameters are pH, hardness, silica and alkalinity (heat exchanger technical guide). To capture 5–10 micron solids, many sites adopt media filtration as side-stream polishing through sand/dual-media filter.

When the particulate load is finer, final polishing is usually done with a cartridge filter. A high-pressure steel housing keeps the industrial operation sound. At the intake or balancing tank, a clarification unit with a residence time of 0.5–4 hours, such as a clarifier, removes more TSS.

Online chemical program (inhibitor + dispersant)

Modern programs combine threshold scale inhibitors and polymer-based dispersants. Low-dose polymers (on the order of ppm) such as polyacrylate/copolymer, with carboxylate, sulfonate, or acrylamide groups, work well for CaCO₃ and other minerals. They work through ion chelation and by disrupting crystal growth (heat exchanger technical guide). These polymers also “distort the crystal lattice”. They usually have surfactant moieties added to help dispersion.

Industry recommendations confirm that good programs pair inhibitors and dispersants. Acrylate acts as a threshold inhibitor and a strong dispersant. It stops micro-crystallites and suspended solids from agglomerating. Adsorbed inhibitor blocks crystal growth. It also disperses particles through electrostatic charge.

Multi-chemistry blends are common. A typical example is 5–20 mg/L polyacrylate copolymer (CaCO₃ control) combined with phosphonate or copolymer for CaSO₄/silica control (heat exchanger technical guide). For CaCO₃, AMP-type phosphonates or polymers are usually used. For CaSO₄, polyacrylate (or AMP) is used. Dosing runs continuously so that near-supersaturated conditions do not end in deposits.

Non-phosphorus “polymer-only” programs are increasingly common (including in Indonesian plants) to avoid the ecological issue of phosphate. Operation at mildly alkaline pH 7–9 also suppresses corrosion. For practical implementation, suppliers usually package the program as scale inhibitors and dispersants specifically for cooling towers. They also supply a package of industrial cooling tower chemical programs.

The base metal still needs protection. Corrosion inhibitors, for example zinc salts, silicates or molybdates, are added according to changes in oxygen and pH. Commercial products are available as corrosion inhibitors.

Operation and monitoring of key parameters

Good flow velocity and turbulence reduce sedimentation. Side-stream filters (sand or cartridge) capture silt before it builds up (power plant case study, POWER Magazine). pH is tightly controlled, usually with sulfuric or carbonic acid dosing, to avoid alkaline hotspots that start Ca-scale nucleation (POWER Magazine, heat exchanger technical guide). Dosing pumps keep the injection accurate so the inhibitor feed stays “just right”.

Conductivity or TDS is used to trigger blowdown before over-saturation. Many plants now set separate limits for conductivity, calcium and hardness, because conductivity alone can be misleading if the raw water chemistry shifts (POWER Magazine). Real-time sensors (online pH, conductivity, ORP, which shows oxidizer status such as chlorine) and lab analysis (hardness, alkalinity) keep inhibitor dosing on target (POWER Magazine).

Biofouling and oxidation control

Microbiological deposits speed up fouling and under-deposit corrosion. Therefore biocide is part of the online program: a routine oxidizer (for example chlorine bleach) combined from time to time with a non-oxidizing biocide (POWER Magazine). Field practice varies: brief shock chlorination with “a few ppm free chlorine for 1–2 hours daily in warm weather,” or low-level continuous dosing (POWER Magazine).

Bleach raises pH and can corrode steel. Therefore many systems add chlorinated isocyanurates or glutaraldehyde when conditions are cooler (POWER Magazine). The biocides package for cooling towers helps keep biofilm under control, so the scale inhibitor works well.

Chemical cleaning during shutdown

If fouling has already formed, periodic cleaning during shutdown restores heat transfer. The cleaning agent depends on the deposit:

For inorganic scale (Ca/Mg carbonate, sulfate, phosphate) and oxide sludge (iron), acids or chelants are used. HCl (hydrochloric acid) or sulfamic acid are common for CaCO₃ and CaSO₄ (heat exchanger technical guide, IntechOpen study on chemical cleaning of heat exchangers). Stronger acids (hydrofluoric acid, H₂SO₄) can dissolve oxides and silica. However, they must be used with an inhibitor and handled with care. Typical recipe: HCl diluted to 1–5% w/w with corrosion inhibitor pellets. Organic acids such as citric acid (usually with hexamine) can also chelate iron sludge (IntechOpen, study of sulfamic acid and citric acid on refinery heat exchanger piping). Note: HF is very effective on iron oxide, but should not be used if calcium exceeds ~1% of the scale mass (IntechOpen). Chelating agents such as EDTA are added for stubborn iron or barium scale (IntechOpen).

For silica or aluminosilicates: these are the hardest. Inhibited hydrofluoric acid-based cleaners (dilute HF) are traditionally used. Alternatively, hot strong alkali (NaOH) plus phosphate can dissolve silicates slowly, usually very slowly. Therefore mechanical methods are usually chosen if severe.

For organic and grease deposits (oil, grease, polymer film), alkaline cleaners with surfactants or chlorinated and aromatic solvents work well. For heavy organic fouling, chlorinated or aromatic solvents are used, followed by washing. Decontamination with a special solvent mixture is usually circulated before the final rinse (IntechOpen, guide to chemical cleaning of refinery heat exchangers).

For carbon deposits (coke, sludge), strong oxidizers or catalytic methods are used. One is hot potassium permanganate (oxidative alkali). The alternative is steam/air decoking. Steam and hot air are injected repeatedly up to the coke temperature to break down carbon through thermal shock, sometimes with a gas scavenger (IntechOpen).

Field execution is done without causing additional damage. Some operators choose third-party services such as cooling tower cleaning service to speed up execution when the system is integrated with a cooling tower.

General procedure, passivation, retesting

In practice, the heat exchanger is isolated, drained, then rinsed. The selected cleaning chemical is pumped through the tubes for several hours and repeated if necessary. It is usually kept below 50 °C to protect the material. All vents and galleries must be included in the circulation. Monitoring flow, pH, conductivity and metal ions in the rinse confirms completeness. After that, a thorough neutralizing rinse is mandatory.

For acid cleaning, standard alkaline passivation is carried out. A mild sodium carbonate (soda ash) mix is circulated to re-form the protective iron oxide layer on steel. This suppresses flash corrosion when the system is refilled (refinery heat exchanger chemical cleaning guide). Finally, the exchanger is pressure-tested, reassembled and returned to service.

Safety, waste, and regulations

Spent cleaning chemicals (acid or caustic with dissolved metals) must be handled according to regulations. In Indonesia, wastewater discharge is regulated by PP No. 82/2001, with limits for pH, TSS, toxic metals and others (peraturan.bpk.go.id). The plant must neutralize and filter the cleaning effluent. It may also need a licensed waste transporter for disposal. A corrosion inhibitor in the cleaning chemical reduces metal dissolution during cleaning. Therefore the downstream treatment load is lower.

Performance metrics and cost impact

Untreated fouling can cut heat-transfer efficiency by tens of percent within weeks to months. However, a well-maintained chemical program can extend cleaning intervals 2–3 times or more. Some plants switched to polymer-based inhibitors and could raise COC by 50% before scale appeared. Studies at power plants note that keeping LSI slightly negative prevents condenser tube scaling and maintains condenser efficiency (POWER Magazine).

Financially, the cost is very material. US estimates show annual chemical spending of ~US$7.3 billion, and ~40% of it goes to scale control in heat exchangers and coolers (IntechOpen). This activity generates >US$2 billion in toxic waste per year (IntechOpen). Preventing just one major heat exchanger shutdown (usually >US$100 thousand in labor and lost production) can fund an inhibitor program for years. Offline cleaning costs are also high. One refinery acknowledges that mechanical cleaning of a large exchanger (disassembly and blasting) can exceed US$60 thousand and 2–3 weeks of downtime. Optimized chemical cleaning (circulation without full teardown) usually cuts 50–80% of that (refinery heat exchanger chemical cleaning guide).

The conclusion is clear. Combine an online antifouling program with planned chemical cleaning during shutdown. The program is [scale inhibitor + dispersant + biocide + corrosion inhibitor](https://beta.co.id/blog/program-kimia-kinerja-untuk-cooling-tower-pabrik-baja-hemat-air-tahan-scale-anti-biofilm). Choose the acid or solvent to match the foulant type. With routine monitoring and precise dosing, this combination gives the most uptime, keeps thermal efficiency, and meets discharge regulations (IntechOpen).