Three levers are cutting energy use in steelmaking: scrap preheating in electric arc furnaces (EAFs), better oxygen blowing in basic oxygen furnaces (BOFs), and waste‑heat recovery from off‑gases and slag. Case studies show double‑digit electricity and fuel savings, faster tap‑to‑tap times, and measurable CO₂ cuts.

Industry: Steel_Manufacturing | Process: Steelmaking

Steelmakers are finding practical gains by reusing heat they already paid for. Preheating incoming scrap to a few hundred degrees Celsius cuts the power bill in EAFs. In BOFs, “post‑combustion” (burning carbon monoxide back to carbon dioxide inside the vessel) puts more heat into the bath. And in both routes, hot gases and molten slag carry energy that can be recovered to raise steam or preheat charge materials.

Across sites and technologies, the pattern is consistent. Kilowatt‑hours per tonne (kWh/t, electricity per tonne of steel), gigajoules per tonne (GJ/t, fuel/heat per tonne), and even tap‑to‑tap time can all fall. Paybacks are usually measured in months to a few years. The data below come from industry reports, peer‑reviewed analyses, and trials (citations inline).

Scrap preheating in EAFs (electric arc furnaces)

Preheating scrap before melting is a mature energy measure. Conventional bucket preheating uses hot off‑gas to warm scrap to about 315–450 °C. It usually cuts electricity by 40–60 kWh per tonne of steel (1library.net).

Modern systems save more. Single‑shaft furnaces (Fuchs‑type) preheat about one‑third of the charge. They can cut EAF power needs by up to ~18% (about 77–110 kWh/t) (1library.net). Continuous feeding systems like Tenova’s Consteel heat scrap counter‑currently with off‑gas on a conveyor. They reach “~~360 kWh/t~~” of total energy use, against ~420–450 kWh/t in older EAFs. That is about 60 kWh/t of savings (www.iipinetwork.org).

In practice, scrap preheating usually cuts specific electricity by 10–25% (for example, 110 kWh/t is ~25% of a 440 kWh/t baseline) and shortens tap‑to‑tap times by 5–8 minutes (1library.net) (1library.net). It also brings other gains. Electrode use drops by roughly 0.3 kg per tonne and refractory use by ~1 kg per tonne (1library.net).

Paybacks are quick. Retrofitting Consteel on a 500 ktpy EAF is cited at about $7.8 per tonne of steel, with savings near $3/t (≈1.3‑year payback). Shaft preheaters can pay back in about one year (www.iipinetwork.org) (www.iipinetwork.org).

In Indonesia, EAFs already use roughly 75% scrap feed. Upgrades like these cut consumption straight away (pmc.ncbi.nlm.nih.gov). Adding heated hot‑metal to the charge (a proxy for scrap heat) cut arc power from 87.4 MWh to 72.9 MWh in an Indonesian 130 t EAF (≈16% cut). CO post‑combustion could trim consumption by a further ~30% (pmc.ncbi.nlm.nih.gov) (pmc.ncbi.nlm.nih.gov).

Optimizing oxygen blowing in BOFs (basic oxygen furnaces)

In a conventional BOF, only about 8–12% of the chemical energy of carbon is captured in the melt. Most of it leaves as CO‑rich gas (www.mdpi.com). Post‑combustion burns CO back to CO₂ above the bath. It captures more heat and shortens blow times.

Dual‑flow post‑combustion lances bring oxygen in through two concentric nozzles. The inner jet decarburizes and the outer burns CO above the bath. CFD‑optimized designs doubled the CO→CO₂ conversion from ≈10% to ≈17% of the CO, and most of the heat went into the steel. This raised BOF thermal efficiency and allowed higher scrap addition (www.mdpi.com). ArcelorMittal Dofasco runs a combined‑blowing BOF, with bottom tuyeres injecting the off‑gas into the shaft. Both scrap charging and post‑combustion increased there. This enabled a 4% higher scrap rate and a matching CO₂ drop (www.mdpi.com) (www.mdpi.com).

U.S. studies estimate that better post‑combustion control could reduce BOF total energy requirements by about 30% (www.iipinetwork.org). Bottom‑gas stirring (submerged tuyeres) lowers flux and oxygen needs and improves yields. In one 80 t BOF trial, optimizing top and bottom lance heights reduced end‑point C and O by ~20% (from 0.0032 to 0.0026) and cut Fe loss to slag by 2.2%. This means less oxidation and less heat loss (onlinelibrary.wiley.com).

Recovering waste heat from hot off‑gases

In EAFs, the hot exhaust (~1,100–1,200 °C) carries roughly 15–30% of the process heat. Mass–energy analyses show a 50–50 mix of chemical heat (from CO) and sensible heat in the gas. For 50% hot‑metal charging, Yang et al. estimate ~274 kWh/t of heat in the gas and another ~43 kWh/t in slag (www.degruyter.com).

Recovering even a portion yields big gains. Waste‑heat boilers or steam cycles on a 150 t EAF can recoup ≈130 kWh/t (at ~30% efficiency) (www.iipinetwork.org). Process simulations suggest a good scheme (combining off‑gas utilities and scrap preheat) could harvest ~170 kWh/t, cutting ~58 kg CO₂ per tonne of steel (www.degruyter.com). In practice, EAF off‑gas heat is used for preheating scrap (as above), raising saturated steam, or driving oxy‑fuel burners. Recovering ~2.8–15.1 MWh/year of electricity from a 150 t EAF is technically feasible (CO₂ savings up to ~12–73 kt/yr). However, this depends on uptime and off‑gas handling (www.iipinetwork.org).

Where waste‑heat boilers are deployed, steam‑cycle reliability depends on make‑up water quality. Plants usually deploy dedicated make‑up treatment, for example a demineralizer, and may dose the steam circuit with oxygen scavengers to protect metallurgy. (Acronyms: CO = carbon monoxide, CO₂ = carbon dioxide.)

BOF gas recovery and mill integration

BOFs also produce large off‑gas flows (~3,000–4,000 Nm³/t, normal cubic meters per tonne) at ~900–1,000 °C, rich in CO. Many plants clean and combust this gas. NEDO (2008) data show 0.125–0.92 GJ/t of BOF gas heat can be recovered via steam or export gas (www.iipinetwork.org).

At ArcelorMittal Ghent, recovered BOF gas replaced about 0.7 GJ/t (≈700 kWh/t) of external fuel. This cut total mill energy use by ~3% (www.iipinetwork.org). Reuse of BOF gas avoids roughly 50 kg CO₂ per tonne of steel. Global reuse could abate ~25 MtCO₂ per year (IEA estimate) (www.iipinetwork.org). Implementation needs scrubbers, cleaning, and onsite power and steam systems. Capital costs can be about $20 per tonne of capacity, with paybacks on the order of a decade (www.iipinetwork.org).

Water‑based gas cleaning trains usually include solids separation. Many flowsheets pair scrubbers with a clarifier as part of the recycle loop. They also use other water‑treatment ancillaries chosen to match local conditions.

Slag heat recovery concepts

Ferrous slags at tapping (~1,200 °C) hold ~1–2 GJ/t of energy (www.mdpi.com). Novel heat‑exchangers (RecHeat designs) can cool slag from about 1,200 °C to ~300–400 °C. They heat air or process fluids from roughly 125 °C to ~340 °C (www.mdpi.com). In theory, oxidizing residual FeO in slag (for example, chemical looping) can also release heat or generate fuel gas.

Slag heat recovery is not yet widespread. However, it could provide tens of kWh per tonne of steel if the heat is captured. For example, each 10% of a 1.5 GJ slag roast is about 150 kWh. Gas heat recovery in boilers or generators and slag heat exchangers together offer one of the largest untapped efficiency gains in steelmaking. They can cut energy use by several GJ/tonne and cut CO₂ at the same time (www.degruyter.com) (www.mdpi.com).

Sources and technical notes

For scrap preheating and EAF data, see industrial surveys and technical reports (1library.net) (www.iipinetwork.org) (www.degruyter.com). For BOF improvements, see Primetals ("Green LD") and iipinetwork summaries (www.mdpi.com) (www.iipinetwork.org) (onlinelibrary.wiley.com). The waste-heat figures come from heat-balance analyses and case studies (www.degruyter.com) (www.iipinetwork.org).