Regulatory targets and raw water

Indonesia is the world’s largest nickel producer and also produces significant cobalt. Wastewater from laterite/leach processing and ferronickel smelters can carry high Ni and Co, usually in the 0.1–10 mg/L range or higher. To protect freshwater, PerMenLingNo. 9/2006 limits dissolved Ni to 0.5 mg/L and Co to 0.4 mg/L in mine wastewater (id.scribd.com). To meet these “polishing” targets, conventional neutralization is not enough. The water needs further treatment.

Raw ferronickelous process waters (RKEF) may carry Ni at tens of mg/L. Typical raw mine waters can have Ni and Co levels orders of magnitude above the regulatory limits. Good polishing is therefore important to avoid violations.

Sulfide precipitation chemistry and performance

Sulfide precipitation removes dissolved Ni²⁺ and Co²⁺ by forming insoluble sulfides (NiS, CoS) when sulfide (for example Na₂S or H₂S) is added, usually at pH 7–9. The solubility products (Ksp, a measure of how readily a solid dissolves) are extremely low, on the order of 10⁻²⁰ for NiS and 10⁻²⁶ for CoS, so most metal precipitates. Tests on Ni-rich effluents (for example 100 mg/L Ni) show 90–95% Ni removal at the best [S²⁻]/[Ni] ratios (iwaponline.com).

Under carefully controlled pH (for example, pH≈5 optimized then raised) and stoichiometry, Ni abatement can reach ~98%. This produces a sludge of millerite (NiS) with some NiO (iwaponline.com). Cobalt behaves similarly and usually precipitates quantitatively as CoS under comparable conditions. In mixed-metal waters, Ni can be less completely removed than more insoluble sulfides (for example, CuS). The kinetics are slower and part of the NiS re-dissolves. NiS tends to re-dissolve under oxygen at pH<10. Therefore systems usually use closed, de-aerated units or rapid solids removal (nepis.epa.gov).

Sulfide trains, cost and constraints

The method is chemically simple and cheap. The reagent costs are low. To precipitate 1 mg Ni (from 1 mg/L feed) you need about 1.3 g Na₂S, priced at about $0.50–1.00/kg. For typical Ni concentrations this comes to a fraction of a cent per m³. The reactions are fast, so the throughput is high. Industrial precedents include processes such as SAVMIN® that use sulfide for precious-metal leachates (pmc.ncbi.nlm.nih.gov). The dose is usually delivered by a metered injection system. In practice, sites pair such metering with a pH control tank and a clarifier, and an industrial dosing pump handles the dosing.

The limits are real. Large reagent doses make a lot of sludge. Every mg of Ni removed makes about 10–20 mg of Ni-containing solid (NiS/CoS mixed sludge). This sludge is usually hazardous. It needs neutralization or landfill, so disposal costs more. Sulfide alone seldom meets tight standards when the influent is high. For a 100 mg/L Ni influent, 94% removal still leaves about 6 mg/L, well above the 0.5 mg/L limit (iwaponline.com). Reviews note that precipitation uses large volumes of chemicals and yields toxic sludge, even though the reagent chemistry is “simple, safe to operate and low-cost” (pmc.ncbi.nlm.nih.gov). The process is complex. It needs precise pH control and there is a risk of NiS re-oxidation. Therefore it needs engineered reactors and reliable settling.

Chelating ion‑exchange polishing

Specialized polymeric ion-exchange resins with chelating functional groups (for example iminodiacetate, bis‑picolylamine) have a very high affinity for Ni²⁺ and Co²⁺. A pilot ran on dilute wastewater, flue-gas desulfurization water with about 0.09 mg/L Ni. A chelate resin (Purolite S930) removed Ni essentially to zero: from 89 µg/L to <0.1 µg/L (>99.9% removal), even with abundant competing cations present (pmc.ncbi.nlm.nih.gov). Such resins usually have high capacity, on the order of 100–200 mg Ni per gram of resin (www.mdpi.com). They work well as a polishing step after bulk removal.

Uptake kinetics for Ni and Co are quite fast (minutes to hours) at mild pH 2–6 (ru.scribd.com). You can tune selectivity by resin choice (thiourea-based resins focus on precious metals, iminodiacetate resins target Ni/Co). Acid stripping regenerates spent resins. This yields concentrated Ni/Co in a small volume, with less solid waste than sulfide sludge. In practice, operators use ion-exchange columns, see Ion-Exchange systems, charged with specialized ion-exchange resins to reach parts‑per‑trillion (ppt) levels if they need to.

Other adsorption media options

Adsorptive media can remove Ni²⁺ and Co²⁺. However, they usually work at lower efficiency than chelating ion-exchange. Activated carbon and modified polymer beads are widely studied. One screening found a carbon resin with Ni capacity of about 144 mg/g, against 90–208 mg/g for several chelating resins (www.mdpi.com). Commercial carbon products, such as activated carbon, can help. However, they usually cannot match the polish of chelate resins.

New materials such as metal-organic frameworks and manganese oxides (δ-MnO₂) adsorb Ni and Co well in the lab, usually by surface complexation. However, they are not yet commercialized for mine effluents. Locally, “green” adsorbents have been proposed, such as rice-husk biochar activated with citric acid. Some report more than 95% Cu²⁺ removal and hundreds of mg/g capacity for Pb, which suggests they may also work for Ni (www.ecoeet.com). However, regeneration, handling (for example silica clogging) and durability in mining waters limit the practical use of these biosorbents. By contrast, ion-exchange resins are mature for metal recovery, for example Dowex M4195 for Ni separation in battery recycling.

Capital and O&M comparisons

Sulfide precipitation needs little specialized capital. The equipment is an injection system, a pH control tank and a clarifier. The reagent cost is very low. Na₂S is ~$0.50–1.00/kg. Precipitating 1 kg Ni needs ~1.3 kg Na₂S, so the chemical cost is ~$0.65–1 per kg‑Ni removed. For typical Ni ~10 mg/L, that is ~$0.01–0.05 per m³ of treated water (www.mdpi.com; iwaponline.com).

Ion‑exchange needs higher capital: a few resin vessels or columns, and roughly 10–20 L of resin for every few cubic meters of throughput. Chelating resins run about $18–70 per liter (www.mdpi.com). 1 m³ of resin (nearly 800 kg) costs ~$18,000–$70,000 up front. One liter can bind many tens of grams of Ni before regeneration. Regeneration needs acid and alkali, and it gives a spent regenerant brine that must be managed.

Performance, polishing and hybrids

Sulfide works best for bulk removal. It drops Ni from 100→~10 mg/L (≈90% removal) at pennies per m³. However, reaching 0.5 mg/L Ni by precipitation alone can need multi‑stage dosing or excess sulfide, and that creates more sludge. Ion‑exchange costs more but gives effluent far below discharge limits. One pilot showed Ni “almost totally removed” to <0.1 µg/L (pmc.ncbi.nlm.nih.gov). The practical strategy is hybrid. Sulfide or hydroxide precipitation does the bulk removal, then ion‑exchange or adsorption polishing reaches the regulatory targets (pmc.ncbi.nlm.nih.gov; iwaponline.com).

In numbers, precipitation might cost about $0.05–0.10 per m³, mostly for reagents, to remove >90% Ni/Co. Ion‑exchange O&M, which covers regeneration chemicals and electricity, might add about $0.20–0.50 per m³. Precipitation alone most likely cannot reach the <0.5 mg/L targets from typical mine water. Ion‑exchange can do so easily, with reported levels <0.001 mg/L (pmc.ncbi.nlm.nih.gov).

Environmental and safety considerations

ChatGPT Image Feb 23, 2026, 11_08_30 AM

The toxicity and volume of precipitate disposal is a major hidden cost. Toxic sludge (NiS, CoS) must be dewatered and usually stabilized or landfilled, with associated fees (pmc.ncbi.nlm.nih.gov). Ion‑exchange’s waste stream, the regenerant acid, is smaller in volume (tens of liters per cycle) but concentrated in Ni/Co. It can be neutralized or processed for metal recovery, potentially offsetting costs. On‑site handling of H₂S or NaHS, if used, also poses safety concerns for sulfide methods.

Throughput and footprint matter. Resin systems are compact, with no large settling ponds, and they run continuously. However, they need careful monitoring for exhaustion.

Data‑backed takeaways

A pilot-scale comparison showed that a H⁺-form iminodiacetate resin (Purolite S930) brought Ni down to virtually undetectable levels. A simple sulfide dose in a batch test left residual Ni on the order of mg/L (iwaponline.com; pmc.ncbi.nlm.nih.gov). Resin costs an order of magnitude more than sulfide chemicals (tens of USD per liter vs cents per kg) (www.mdpi.com). However, the resin gives water quality that easily meets SNI/National Class C standards.

In the end, the choice depends on the effluent quality you need and the cost. In Indonesia, the tight 0.5/0.4 mg/L Ni/Co limits mean a polishing step after primary treatment is almost always needed, for example ion exchange or adsorbents (id.scribd.com).

Sources and references

Peer‑reviewed studies and industry reports underpin these findings. Performance data draw from waste‑treatment research (Jerroumi S. et al., Water Quality Research Journal 55(4):345–356, 2020—Ni sulfide precipitation experiments—iwaponline.com; iwaponline.com) and review articles (Matebese F. et al., Heliyon, 2024—mine water tech review—pmc.ncbi.nlm.nih.gov).

Czupryński P. et al., RSC Advances 12:5145–5156 (2022)—pilot ion‑exchange removal of Ni/Hg/Cr—pmc.ncbi.nlm.nih.gov. Z. Zainol & M.J. Nicol, Hydrometallurgy 96:283–287 (2009)—chelating IEX for Ni/Co; ammonium vs H⁺ forms—ru.scribd.com. Wołowicz A. & Z. Hubicki, Processes 9(2):285 (2021)—resin screening; costs and capacities—www.mdpi.com; www.mdpi.com.

Indonesian MoE Permen No. 09/2006—wastewater standards for nickel mining—id.scribd.com. Woolsey S.E. et al., Mine Water Environ. (EPA Report, 1986)—sulfide precipitation kinetics: NiS dissolution—nepis.epa.gov. Additional context on SAVMIN® and precipitation trade‑offs appears in Heliyon (2024) (pmc.ncbi.nlm.nih.gov).