Hot-rolling mills used to run on "once-through" water. Now they recirculate it. With scale pits, oil-water separators and multi-stage filtration they cut freshwater by 70–90%, and the spray nozzles stay clear and the strip quality stays stable.

Industry: Steel_Manufacturing | Process: Rolling

Steel rolling mills use vast quantities of cooling water. Depending on recycling practice, total intake ranges from less than 1 up to about 150 m³/t (cubic meters per tonne) of steel (worldsteel project). In well‑recycled integrated mills, common intake is around 5–30 m³/t because roughly 85–90% of process water is reused or returned (IspatGuru, MDPI). Older once‑through systems can consume hundreds of m³/t. In practice, closed‑loop cooling can cut freshwater use by 70–90% under drought or regulatory pressure.

Hot-rolling lines usually run two water circuits. The first is an open "contact" loop. Here the sprays hit hot steel directly and pick up heat, iron-oxide scale and lubricating oils. The second is a sealed "non-contact" loop for exchangers, hydraulics and machinery. This water never mixes with process water (rolling-mill water treatment study). The closed-loop design treats the contaminated contact water so it can be reused. Therefore the mill discharges less.

Contact and non‑contact circuits

In the open (contact) circuit, high-pressure descaling jets strip iron-oxide scale and roll-cooling water washes off solids and oils. Both return to treatment. The closed (non-contact) circuit cools equipment through heat exchangers. Therefore the water stays clean enough to recirculate (same study).

Scale pits and sedimentation basins

All runoff first drops into large scale pits (open sumps where heavy solids settle by gravity). Mill scale is dense (≈7.65 g/cm³) and forms continuously, at roughly 0.1–0.3% of rolling throughput. Therefore good settling is important. One case cites a 90 t/h rolling train producing 18 kg/h of scale. This guides pit sizing and solids removal (rolling‑mill water treatment study).

Designs usually specify about 30–45 minutes of residence time, with scraper pans or conveyors removing settled solids (WesTech flow sheet). Multistage decantation is common. Heavy scale drops out in the pits (and any upstream reception pools). Then clarified water overflows to secondary clarifiers to capture finer grit (sedimentation detail). Plants usually use a clarifier for secondary settling to stabilize turbidity before downstream steps. If scale is not removed early, it remains suspended and later clogs spray headers or fouls heat exchangers.

Oil–water separation equipment

After sedimentation, water flows into oil‑removal units. Contact water always picks up tramp oils (leaked hydraulic fluids and roll oils). Between pits and clarifiers, flotation causes oils to rise, where mechanical skimmers or coalescer units strip them off (WesTech, Filternox). In one configuration (In [27]), the scale pit itself integrates an oil skimmer and scraper to float off oil while settling solids.

Loads can be significant. One industry case reports up to 40 L/h of oils/grease entering a large hot strip mill’s circuit (case data). Good separators push residual oil down to a few ppm (parts per million). Many systems reach final oil‑in‑water at about 10–50 mg/L. Mills usually standardize on oil skimmers or automatic oil‑water separators (plate‑coalescer tanks or SAS systems) built to handle sudden surges. Plants do this step with dedicated equipment such as an oil‑removal separator to protect downstream filters from fouling (WesTech, Filternox).

Filtration and polishing stages

After separation, water still carries fine particulates and trace oil. Treatment trains use deep‑bed sand or multimedia filters, self‑cleaning automatic strainers, or pressure‑cartridge filters. One supplier’s flow sheet routes pretreated water through deep‑bed sand filters to trap fine iron oxides and coalesce remaining oil (WesTech). In a hot‑rolling case study, water after oil separation flows through two sand filters before reuse (MDPI case). Plants usually add a self‑cleaning step with an automatic screen filter to intercept grit surges before media beds.

Pretreatment usually has 200 µm then 50 µm security filters in series ahead of ultrafiltration pilots (MDPI pilot). Many mills use sand media such as silica sand and top layers of anthracite to deepen filtration. Cartridge stages are also used for fine polishing. A cartridge filter gives a predictable micron cut for nozzle protection.

Self‑cleaning filters backwash automatically, so they do not clog. Their sludge is about 2–5% of flow. It is recycled to the scale pit, or thickened and dewatered. In one design, filter backwash goes to a thickener and filter press, and the clarified effluent is recycled to the pit (WesTech design note). When membrane polishing is piloted, ultrafiltration (UF) benefits from those 200 µm → 50 µm “security” filters upstream. UF is a pressure‑driven membrane step that sieves out very fine particles and emulsified oils (MDPI pilot).

Closed‑loop recirculation and makeup

After filtration, the water is essentially free of visible solids and oil. It is collected in a surge tank, usually ahead of cooling towers. It is pumped back to spray headers and cooled via towers or heat exchangers to the target spray temperature. The system is closed, so only makeup water for evaporation and bleed‑off is added. In well‑engineered loops, makeup is usually 2–5% of flow (rolling‑mill water treatment study). An open loop, by contrast, would need 20–50× more freshwater.

Nozzle fouling and equipment impacts

We control solids and oil for a simple reason. Even a small amount of debris or oil will cripple a closed loop. Scale fines and gelled oil clog nozzles and filters. Then the jets become uneven, strip cooling gets poor and surface defects appear. One filter supplier says: “If cooling water contains particles which clog the spray nozzles, this will lower the quality of the end product… and lead to serious losses in production” (Filternox).

Modern mills usually specify in‑nozzle mesh screens or very fine filters. For example, tungsten‑carbide descaling nozzles have internal stabilizing filters that catch particles which slipped past plant filtration (Sealpump). Oil and grease make screens foul faster. "High energy back‑flushing" filters are used to avoid blockage from oils (Filternox). Scale or oil that is not recovered forces extra downtime to chemically clean or replace clogged nozzles, blades and pipes. This interrupts production and wastes water (loop flushing) and energy (reheating after shutdown).

Dissolved salts and deposition control

Dissolved salts and minerals also concentrate through evaporation. They are not particulates or free oil, but they must be managed so that they do not deposit on rolls and equipment (MDPI). However, particulate scale and oil are the immediate foulants. They are what drives nozzle and heat‑exchanger reliability.

Performance metrics and savings

With pit‑separator‑filter trains that work well, many steel mills now [recycle ≥95% of their water](https://beta.co.id/en/blog/steels-water-rethink-how-closed-loop-circuits-in-hot-rolling-mills-hit-9098-reuse-and) (SBQ Steels). A worldsteel survey has recorded specific water intake as low as under 1 m³/t in plants that recirculate very heavily (worldsteel project). The benefits are direct: lower utility bills, reduced effluent, longer equipment life (less corrosion/scaling), and more consistent cooling.

The loads show what is at stake. In a 90 t/h mill, up to 18 kg/h of iron oxide can enter the cooling stream (rolling‑mill solids data). Up to 40 L/h of lubricating oil can come in with it (oil load case). Pits and separators capture these, so the load on spray headers and pumps stays very low and rolling can run without a stop. Continuous skimming and sedimentation keep filtration from clogging and prevent damage to the machinery, so the plant runs better (Oil Skimmers, Filternox).