Article
Steel’s hot problem: How cokemaking is turning wasted heat into steam, power, and cash
Waste Heat into Power: How Coke Plants Turn Efficiency into Electricity and Steam
Coke oven batteries have a large efficiency gap. Flue gas heat recovery and Coke Dry Quenching (CDQ) can raise energy utilization from about 55–60% to about 82–89%. They also cut emissions and fuel bills.
Behind the gleam of steel, the coke line is a large heat engine. To produce 1 ton of metallurgical coke, the process uses about 1.37 tons of low-ash, low-sulfur coal (heattreatconsortium.com). However, most of the energy stays in the product. About 68% of the coal's energy ends up as sensible heat in the coke, about 12% in the by-product gas, about 12% in tar/oil, and only about 8% is burned as internal fuel (heattreatconsortium.com).
The direct heat demand of the coking process itself (pyrolysis, heating without oxygen) is only about 3.2–3.4 MMBtu (3.4–3.6 GJ) per ton of coke. MMBtu is a million British thermal units. GJ is gigajoule (heattreatconsortium.com). However, studies show that only 51.2% of the fuel energy is used for carbonization. The rest is lost through flue gas, radiation, wall losses and quenching (stet-review.org). Industry surveys estimate that losses through flue gas alone can be about 17% of the heat output (steeljrv.com).
The thermal efficiency of coke ovens today is in the 55–60% range. Therefore the gap for energy recovery and reuse is still wide.
Energy balance in a coke oven battery
Modern coke oven flue gas is usually at 180–300 °C. One analysis shows that cooling flue gas from ~850 °C to 450 °C through an evaporator can recover ≈4.39 GJ per battery cycle (about 6.5% of input energy) (stet-review.org). Preheating combustion air with this heat saves a further ~4.65 GJ (about 6.9% of input energy). It can also raise overall thermal efficiency to ~58% (stet-review.org).
In practice, the flue gas heat goes to a waste-heat boiler to make high-pressure steam (HP steam). A real example comes from the “CDQ power island” project. Two ~60 t/h HP boilers plus one existing 75 t/h boiler supply about 145 t/h of steam to the turbine, generating about 40 MW of electricity (tce.co.in). Boiler feedwater quality matters here. If the TDS is high, the boiler scales and corrodes. Many facilities use pretreatment such as reverse osmosis to lower TDS before the boiler, for example a brackish water reverse osmosis system for utility supply, then supplement it with an industrial boiler chemical program to control scale, corrosion, and dissolved oxygen.
After RO, a deionization unit helps reduce the remaining ions so the boiler stays stable and clean. In many industrial utility assets this is done with cation/anion demineralizers to keep conductivity and silica within the safe range for the steam cycle.
Coke Dry Quenching and heat recovery
Wet quenching sprays energy into the air as steam. Coke Dry Quenching (CDQ) works differently. It cools hot coke by circulating inert gas in a heat exchanger, and it captures the coke's sensible heat as HP steam (kep.idaminfra.com). In practice, CDQ can capture about 24% of the coke's energy content (stet-review.org).
Wet quenching needs about 0.6 MMBtu (≈0.63 GJ) of steam per ton of coke. CDQ produces more than enough steam for process needs and can still export the surplus (heattreatconsortium.com) (heattreatconsortium.com). One analysis predicted that CDQ can push oven efficiency to 82%, and up to 88.6% when gas heat recovery and extra insulation are added (stet-review.org).
The scale is significant. Combined with exhaust gas heat recovery, one battery of 70 ovens can potentially save ~617,000 GJ/year (stet-review.org). Implementation is already widespread. Many steel plants in Japan, China, India, and Finland have installed CDQ with steam turbines, usually as part of carbon reduction programs (ctc-n.org) (ctc-n.org). In Finland, the Rautaruukki facility reports CDQ utilization >99.6% with average uptime of ~85–90% (ctc-n.org).
In the CDQ steam cycle, water/steam management affects turbine and heat exchanger reliability. Many operators “polish” the condensate after the heat exchanger through a condensate polisher unit to keep TDS/silica very low. Boiler chemical programs are also common. These include boiler condensate chemical treatment and dissolved oxygen reduction using oxygen scavengers to reduce corrosion in steam pipes and drums. For conductivity and silica control in the steam cycle, industrial boiler water chemicals are also available.
Heat recovery and emissions impact
Waste gas heat recovery and quench heat recovery do two things at once: they save fuel and they lower CO₂. One study estimates that combining the two can save about 25.2 GJ per batch, cut CO₂ by about 2.45 ton per cycle, and give a value of about $233 per cycle from carbon credits (stet-review.org). In engineering practice, similar projects also show a combined valuation of increased heat recovery of about $2,578 per oven cycle, with a CO₂ reduction of about 2.45 ton in the same cycle (stet-review.org).
Here is another example from the generation side. At an integrated plant, a CDQ boiler produces about 145 t/h of HP steam. That steam drives a turbine of about 40 MW. The power comes from waste heat (tce.co.in).
Oven heating fuel: options and reality
Coke ovens are usually heated by burning by-product gas in the heating flues. The main fuel is coke-oven gas/COG, the gas generated from coal carbonization. Many modern facilities use a mix. COG supplies about 40% of the heat, and the rest is recycled back to the oven (heattreatconsortium.com). At peak load, or when gas is short, natural gas or light fuel oil helps stabilize the heat supply.
One domestic case is worth noting. At Krakatau Steel (Cilegon, Indonesia), a new oven design captures all COG and uses it on site. This reduces the consumption of expensive pipeline gas in reheating furnaces and boilers. Management estimates savings of about US$60 per ton of HRC product (ekonomi.bisnis.com). The release stated that “coke oven gas … replaces natural gas (which is more expensive) as fuel in reheating furnaces and boilers” (ekonomi.bisnis.com).
Low-carbon options are starting to be studied. Hydrogen-rich syngas or “green” hydrogen can in principle be burned in oven burners to reduce CO₂ emissions. Furnace modernization programs in Europe/Japan are developing burners for “lean gases” mixtures (gases with low calorific value), including hydrogen. Biomass-based syngas or bio-steam reforming of heavy oil may also be explored. However, scale and coke quality limitations mean adoption will not be quick. There is also the concept of co-producing synthetic fuels. For example, CO₂ from coke oven gas can be recycled into SNG or DME (dimethyl ether) for reuse in the oven or other units. Indonesia itself is exploring coal-to-DME for cooking fuel (aseanenergy.org).
Under current technology conditions, economics mainly decides how the furnace fuel is diversified. If COG is abundant, it usually covers 80–90% of heat demand, in practice as "free fuel" from the process. Alternatives must compete on cost or environmental benefit. [Natural gas remains the most common supplement](https://beta.co.id/blog/tanur-tiup-makin-irit-pci-gas-alam-dan-ccs-memotong-kokas-dan-co2-di-pusat-baja). Options such as [hydrogen burners](https://beta.co.id/blog/ladle-furnace-lebih-irit-energi-insulasi-kontrol-listrik-dan-burner-h2-mulai-mengubah) are still mostly R&D. Biomass gasification is less practical at steel plant scale. With blend adjustment (for example adding 20–30% additional gas), small savings of a few percent can be significant financially and in carbon terms. To keep utility chemical operations consistent, precise chemical injection is usually carried out through dosing pumps in boiler and condensate networks.
Summary of energy and utility impacts
In short, exhaust-gas heat recovery can return an additional ~6–7% of input energy, about 4–5 GJ per batch (stet-review.org) (stet-review.org). CDQ recovers ~24% of the coke's sensible heat (stet-review.org). Together, the two can more than double the oven's "used" energy, from ~51% to ~82–89% (stet-review.org). That saves about 25 GJ of fuel per cycle and hundreds of thousands of GJ per year per battery (stet-review.org).
On the fuel side, using more byproduct gas, including BF gas (blast furnace gas) when it is available, already reduces the need for purchased fuel. Experience in Indonesia and internationally shows that recovering COG for internal heat can save tens of dollars per ton of steel (ekonomi.bisnis.com) (ekonomi.bisnis.com). Dozens of steel plants have installed waste‑heat boilers and CDQ. The payback time is usually a few years. For example, a project supplies 145 t/h of HP steam to a ~40 MW turbine (tce.co.in).
The statistics and analysis come from authoritative sources and peer-reviewed studies on energy flows and coke technology (heattreatconsortium.com) (stet-review.org) (stet-review.org) (stet-review.org). They also come from case studies (for example TCE/Tata and Krakatau Steel) and CDQ reviews (ctc-n.org). The findings are drawn from recent literature and industry reports (2021–2025) on coke efficiency.