Inside the race to re‑tune the blast furnace: PCI, natural gas, and CCS
Inside the race to re‑tune the blast furnace: PCI, natural gas, and CCS
The blast furnace still makes about 70% of the world's steel, and most of its CO₂. Plants now use pulverized coal and natural gas injection, and they look at carbon capture next, to cut fuel and emissions without stopping the iron flow.
Blast furnace ironmaking (BF) is still the industry's workhorse. About 70% of global steel comes from the BF/basic oxygen furnace (BOF) route (ResearchGate) (ResearchGate). That dominance comes with a carbon bill: ≈2.0–2.2 tonnes of CO₂ per tonne of hot metal (tHM, the liquid iron tapped from the furnace) (ResearchGate). That is ~2.6 Gt CO₂ per year, around 7% of global emissions (ResearchGate).
About 70% of steel's CO₂ comes from the BF itself (Carbon Capture Journal), so even small efficiency gains matter. A typical BF uses about 13–14 GJ/tHM (ResearchGate). Operators are pushing the core thermodynamics with hot‑blast stove optimization, [top‑gas recovery turbines](https://beta.co.id/en/blog/steels-dirtiest-stream-is-now-a-fuel-inside-the-blast-furnace-cleanup-that-pays-for-itself), oxygen enrichment, and fuel replacement through tuyère injection (the nozzle region where the hot blast enters).
Blast‑furnace energy and emissions baseline
The traditional BF/BOF route gives off more emissions than electric-arc steelmaking. Therefore the fuel mix and [heat recovery](https://beta.co.id/en/blog/steels-hidden-furnace-how-coke-ovens-can-turn-waste-heat-into-steam-and-power) are important levers (ResearchGate). Two injection strategies dominate the optimisation work today: pulverized coal injection (PCI) and natural-gas (NG) injection. A third, carbon capture and storage (CCS), is the deep-cut option for the concentrated CO₂ streams of the BF.
Pulverized coal injection (PCI) performance
PCI feeds fine coal pneumatically through the tuyères. The coal supplements metallurgical coke as both fuel and chemical reductant. Use is widespread. Estimates suggest at least 65% of blast furnaces use injection, and about 75% of the injection BFs use coal (ResearchGate) (ISIJ International).
The displacement effect is the big gain. Industry data put the coke replacement of PCI at about 0.85–0.95 tonnes of coke per tonne of injected coal (IIP Network). One data point: 1 tonne of PCI coal has been noted to displace about 1.4 tonnes of coking coal, which points to about 30% coal savings (Docslib).
Worrell et al. estimate that about 3.76 GJ of energy is saved per tonne of pulverized coal injected (IIP Network). Globally, lifting average PCI to about 180 kg/tHM could cut on the order of 10 Mt CO₂ per year (IIP Network) (IIP Network). In practice, many furnaces now inject 100–180 kg/tHM and trim coke by about 15–30%. For example, a 400 kg coke/tHM furnace drops toward about 280–340 kg/tHM at heavy PCI (IIP Network). Each tonne of coke avoided (about 0.85–1.0 t coke per tPC saved) cuts about 2.0–2.5 tCO₂ (about 2.0 t/tHM typical BF emission intensity) (IIP Network) (ResearchGate). Therefore about 1.7–2.4 tCO₂ is reduced per tonne of PC used.
On the ground, PCI rates above 150 kg/tHM are now common in China, India, the U.S., and Europe. Theoretical limits are governed by combustion kinetics and ash behavior. They run ~200–270 kg/tHM (ResearchGate). In China, co‑injection trials (natural gas plus PCI) at Chongqing Iron & Steel improved hot‑metal quality, lowered the coke rate, and lifted productivity (ISIJ International). In the U.S. and Europe, high PCI rates are also reported. POSCO cited average PCI exceeding 150 kg/tHM at its modern Kaldo furnaces.
Coal choice matters. Volatile content and grindability set raceway combustion efficiency. Poor combustion risks unburned char and altered coke behavior in the hearth. The economics usually pencil. U.S. analyses put savings at $16–33 per tonne of hot metal from PCI, roughly 4–5% of HM production cost. Capital is about US$50–55 per annual tonne of injected coal capacity for mills and injection systems (IIP Network). During pulverized coal preparation and conveyance, plants also plan for materials‑handling controls. Some operators evaluate coal‑dust control options alongside PCI system design, including market offerings such as a coal‑dust suppressant.
Bottom line: under heavy PCI, typical BF coke usage can drop ~20–30%. A 2010 EPA guide summarized that ~25–30% of BF coal demand can be saved via PCI (≈0.9 t coke avoided per tPC) (IIP Network). Every kilogram of coke saved avoids about ~3.0 kg CO₂.
Natural gas injection and oxygen enrichment
Natural gas (CH₄) or other hydrogen‑rich gases, for example coke oven gas or syngas, can also be injected at the tuyère. In the raceway, CH₄ reforms endothermically to CO+2H₂. This supplies ash‑free reductants and changes the flame temperature and the gas composition. In trials, NG injection rates are usually 20–100 m³/tHM. Use rises where gas is inexpensive (ISIJ International).
Modeling by Li et al. (2025) shows the scale of the effect. Adding 100 m³/tHM of NG with 6% oxygen enrichment and decreasing PCI cut the coke rate by ~21 kg/tHM and reduced CO₂ by ~60 kg/tHM (ISIJ International). In that scenario, 100 m³/t displaced about 62 kg/t of PCI and reduced coke by 21 kg/t. Therefore the lower coke and PCI levels save ~2.2 tCO₂ per tHM indirectly (ISIJ International). Other studies cited find roughly 4–6 kg of coke saved per extra 5–10 m³ of NG injected (≈0.8–1.2 kg coke per m³ NG) (ISIJ International).
NG cools the raceway because the reforming is endothermic. Therefore operators boost blast oxygen or preheat the NG. Co-injection with PCI widens the operating window. Oxygen enrichment alone (about 2% more O₂) can cut the coke rate by about 3% (≈25 kg/tO₂ per 100 kg coke) (ISIJ International). This allows higher NG shares. Case experience, for example Chongqing Iron & Steel, reported better hot-metal quality and lower coke rates with modest NG injection (ISIJ International).
The carbon math shows the trade-offs. On a per-carbon basis, 1 kg of CH₄ roughly replaces 1 kg of carbon from coal. If it is fully combusted, it yields about 2.75× less CO₂. Therefore 100 m³ (≈80–90 kg) of NG replaces ~80–90 kg of C and saves ∼220–250 kg CO₂ versus coal. In the cited modeling, the co-injection/oxygen-enriched setup delivered ~60 kg CO₂/tHM saved for 100 m³/t (ISIJ International). This reflects the partial substitution and the reduced PCI. In practice, high-NG systems (≥50–100 m³/tHM) usually lower coke use by ~5–10% when they are coupled with oxygen enrichment.
Carbon capture and storage (CCS) feasibility
Even with PCI and NG, BFs emit ≈2+ tCO₂/tHM. Post-combustion CCS is the main pathway to deep cuts. Capturing BF CO₂ targets roughly 70% of a steel plant's emissions (Carbon Capture Journal). At an integrated site (coke ovens, sinter, BF), those BF-related processes can run to about 80% of site CO₂. BF top gas (usually 20–25% CO₂) and hot-blast stove flue gases are attractive capture targets. Chemically scrubbing the BF gas at ~90% capture would cut integrated plant CO₂ by ~63% (0.9×0.7) (Carbon Capture Journal).
The technology is new in steel. As of 2024, only two carbon‑capture projects operate in the sector (≈1% of capacity). Just one BF‑BOF CCS scheme is planned, against dozens of hydrogen‑based projects (Transition Asia). Costs are a hurdle. Retrofitting a BF can run ~$50–100+ per tonne CO₂ captured (IEAGHG studies vary). However, pilots show promise. An ArcelorMittal/Sekisui trial processed real BF gas in Spain. It reached ~90% CO₂ purity in capture and 90% conversion efficiency, so the process is technically feasible (Carbon Capture Journal).
Energy and site integration matter. Full BF CCS can theoretically cut plant CO₂ by about 60–80%. In practice, capture would target BF runner gas and possibly converter gas stacks. With the right stove configurations, for example oxygen‑fired stoves, a site reduction above 50% is plausible. The BF makes up about 70% of site emissions. Capturing 90% of that share alone gives about a 63% site reduction (Carbon Capture Journal). Coke ovens and reheating still leave residual emissions. Therefore CCS is important for deep decarbonization. Chemical scrubbing units need solvent management. Operators usually provide accurate chemical metering and corrosion control in these loops. Utilities such as a dosing pump and a corrosion inhibitor may be specified in the balance of plant.
Policy is catching up. CCS needs a lot of low‑grade heat, usually met by steam extraction, and the capex is high. Therefore deployment to date is limited to models and small pilots. Few jurisdictions mandate CCS in steel. Indonesia is one to watch. Presidential Reg. 14/2024 and MEMR Reg. 16/2024 (effective December 2024) set permits for carbon storage areas (WIPKs). This lays the legal groundwork for future CCUS across sectors, possibly including steel (Ashurst). Some projects with chemical scrubbing capture trains also plan upstream gas‑cleanup or solvent handling consumables. Vendors market CO₂/H₂S removal solvents such as amine systems as part of generic gas‑treatment toolkits.
Economics, policy signals, and next‑decade outlook
Today’s gains are incremental but material. PCI remains a “low‑hanging fruit”. Heavy injection cuts coke by ~20–30%. Each tonne of PC injected saves ~3.76 GJ of energy. If average PCI reaches ~180 kg/tHM, global abatement could be on the order of 10 Mt CO₂/yr (IIP Network). NG co‑injection (usually 20–100 m³/tHM) brings 5–10% coke savings at high injection levels when tuned with oxygen enrichment. Modeling examples show ~60 kg CO₂/tHM reductions for 100 m³/t plus 6% O₂ (ISIJ International).
CCS is the lever for deep cuts. With BF gas capture it can give site reductions of more than 50%. However, it sits early on the cost and policy curve (Transition Asia) (Carbon Capture Journal). Regulatory frameworks such as Indonesia's new carbon storage rules are still maturing (Ashurst). As they mature, capture projects will have clearer permitting paths. Until then, blast-stove efficiency, top-gas recovery, oxygen enrichment and tuned injection mixes will carry most plants' energy-efficiency and emissions-intensity goals. Operators who upgrade utility blocks around these projects need the usual industrial housekeeping, from conveyance dust control to routine water and chemical handling across the site's auxiliaries.
Sources: Efficiency and injection figures: (IIP Network) (ISIJ International) (ResearchGate) (ResearchGate). Emission shares: (ResearchGate) (Carbon Capture Journal). Economics and regulation: (IIP Network) (Ashurst).