Article
Galvanizing’s zinc problem meets a conventional fix: filtration, pH 9–10, clarification
Galvanizing’s zinc problem meets a conventional fix: filtration, pH 9–10, clarification
Hot-dip galvanizers send 0.5–3.0 m³ of water per tonne of steel through quench tanks. They then have to strip zinc to low mg/L. A three-step design does this: physical filtration, hydroxide precipitation and clarifier settling. It delivers >90% removal and routinely hits <5 mg/L Zn.
Hot‑dip galvanizing uses a lot of water, about 0.5–3.0 m³ per tonne of steel, to quench or clean zinc‑coated steel (iwaponline.com) (iwaponline.com). Worldwide, about 60% of the ~13 million tonnes of Zn produced per year ends up in galvanizing. That is about ∼72–75 kg Zn per tonne of steel (iwaponline.com).
Cooling and rinse tanks alone use ~2,300 L freshwater per tonne (≈2.3 m³/t, iwaponline.com). Most of that, 95%, becomes wastewater (~400–3000 L/t steel, iwaponline.com). The quench effluent usually carries zinc as fine particulates (scrap, spatter) and dissolved Zn (usually 10–100’s+ mg/L). It also carries other metals (Fe, Cu, etc.) and a high pH from the alkaline rinse.
One study reported Zn in galvanizing rinses from ~70 up to 33,800 mg/L (iwaponline.com) (iwaponline.com). Indonesian regulations (for example, Permen LH 5/2014) usually limit Zn in effluent to low mg/L (for example, ~5 mg/L or less). Therefore the plant needs more than 90% removal in practice.
Quench effluent loads and target
Designing for the numbers above means removing both suspended zinc particles and dissolved zinc species. The goal is simple: meet low mg/L limits on Zn with a reliable end‑of‑pipe sequence that fits typical galvanizing flows and concentrations.
Coarse‑to‑fine filtration train
The first step is physical filtration to remove suspended Zn particles. Plants usually start with coarse screening around 0.5–1 mm before fine filtration. This protects downstream media because metal hydroxide flocs and zinc spatter clog filters easily (nepis.epa.gov). For coarse solids control, operators usually deploy an in‑channel screen such as a manual screen.
Bag or cartridge filters in the 10–100 µm range capture micron‑scale particulates. Cartridge filters are a common choice as polishing stages that keep headloss low. In practice, well‑designed bag/cartridge systems remove 85–99% of total suspended solids (TSS, the suspended particles measured gravimetrically) and turbidity (www.researchgate.net).
For larger flows, media filters add throughput and resilience. Dual‑media beds such as sand/silica filters handle higher solids loading and keep the effluent clarity stable. Key design numbers: filtrate should reach >90% solids removal. Change‑out frequency depends on the load. Metals‑finishing filters are usually cleaned or replaced when differential pressure (ΔP) reaches ~50–80 kPa.
A real‑world test shows the gains. With alum coagulant, turbidity dropped from 557 to 1.4 NTU (99.7%) (www.researchgate.net). Even without coagulant, particulate Zn can still be >90% removed by proper pore‑size selection. Where plant layouts need an integrated headworks, packaged wastewater physical separation systems provide screens and primary solids removal upstream.
Hydroxide precipitation chemistry
Dissolved Zn²⁺ is removed by pH adjustment. The pH is raised to 8.5–10 to form zinc hydroxide (Zn(OH)₂, an insoluble precipitate). Zinc hydroxide solubility is lowest around pH ≈9–10. For most zinc systems, precipitation is essentially complete by pH 9.0–9.5 (www.researchgate.net). Plants dose caustic alkali, NaOH or Ca(OH)₂, through a metered system such as a dosing pump to reach ~pH 9–10, depending on the buffering.
Bench data show that raising the pH to 9.5 with the right coagulant can drop Zn from ~80 mg/L to ~3.7 mg/L (95.3% removal) (www.researchgate.net). Even pH≈9.0 gives ~93.8% removal (effluent Zn <5 mg/L) (www.researchgate.net). For perspective, an EPA example notes that adjusting a metal‑rich stream to pH 9 would reduce dissolved lead to ~0.2 mg/L versus 0.8 mg/L at pH 7.5 (nepis.epa.gov).
Dosing follows stoichiometry: roughly 2 moles of OH⁻ per mole Zn to form Zn(OH)₂. In practice, the alkali requirement is usually on the order of 100–300 mg NaOH per liter for wastewater with tens of mg/L Zn, depending on initial pH and buffer capacity. To agglomerate fine Zn(OH)₂ flocs, plants add iron or aluminum salts from a coagulants program, sometimes supported by a flocculant polymer.
One study found that a low alum dose (50–150 mg/L) plus 10 minutes of mixing improved clarity and removal a lot (www.researchgate.net). Typical hydraulics use rapid mixing for 30–60 seconds, then slow mixing for 5–10 minutes. This lets the precipitate form and the floc grow.
Clarifier sizing and performance
After precipitation and flocculation, the slurry flows to a clarifier (sedimentation tank). The clarifier separates zinc hydroxide sludge from clarified water. A hydraulic retention time of 0.5–2 hours is common for metal‑hydroxide settling. The surface overflow rate is usually kept at ≤ 0.05–0.2 m³/m²·h (360–1,440 m³/m²·d) so the floc can settle.
As an example, at 0.1 m³/m²·h, a 10 m³/h flow needs ~100 m² of area (10 m² per 1 m³/h). In practice, much lower surface loading (for example, 0.01 m³/m²·s, or 0.36 m³/m²·h) is used for fine precipitates. The weir overflow rate should be <0.5 m³/m²·h to prevent carryover. A conventional clarifier gives the detention time and solids control this duty needs.
Where space is limited, plate clarifiers can save footprint. A lamella settler gives the same separation in a compact plan area. A tube settler raises clarifier capacity by adding effective settling surface.
With well‑formed flocs, clarifiers can remove >95% of precipitated Zn(OH)₂. In the literature, combined flocculation/clarification routinely achieves >90–95% Zn removal (www.researchgate.net) (www.researchgate.net). One study reports final effluent Zn ~3–4 mg/L after full clarification (www.researchgate.net) (www.researchgate.net). Residual TSS in clarified effluent is usually <10–20 mg/L, and usually <5 mg/L.
Sludge handling and yield
The clarifier bottom yields zinc hydroxide sludge that is gelatinous. Thickening and dewatering are recommended. A belt or plate press can dewater the sludge to >20% solids for disposal or zinc recovery.
A simple yield estimate helps size the handling systems. Removing 1 kg of Zn yields ~1.6 kg Zn(OH)₂ (molar mass 99 vs Zn 65, so sludge weight is ~2.5× Zn mass). For example, 80 mg/L Zn in 100 m³ gives ~8 kg Zn (as ≈20 kg Zn(OH)₂) in the daily sludge.
Outcomes, compliance, and figures
Combined treatment, which means [filtration plus precipitation plus settling](https://beta.co.id/en/blog/inside-a-galvanizing-plants-quench-tank-fix-filters-highph-chemistry-and-a-clarifier-that), can reduce Zn from tens of mg/L down to below discharge limits. A lab‑scale treatment cut Zn from 79 to ~3.7 mg/L (95.3% removal) (www.researchgate.net). Even at pH 9.0, removal reached 93.8% (≈4.9 mg/L) (www.researchgate.net). After treatment the pH is adjusted (neutralized) to meet discharge rules in the 6.0–9.0 range. Most plants do this with water‑treatment ancillaries.
Other dissolved metals and contaminants (Cu, Fe, etc.) also precipitate at the same pH range. This gives multi‑metal removal (www.researchgate.net). In full‑scale HDG facilities using conventional end‑of‑pipe treatment (coag‑floc, sedimentation, filtration), cooling rinse streams at ~98–272 mg/L Zn enter treatment and discharge at ~<10 mg/L (iwaponline.com). EPA plating guidance likewise presumes hydroxide precipitation can meet limits. This reflects its status as “best practicable technology” (nepis.epa.gov).
The key design figures sum up the approach. Use a chemical dose of around ~200–300 mg/L Ca(OH)₂ (or equivalent NaOH) for 50–100 mg/L Zn. Set the pH to ∼9.0–9.5, as the solubility chemistry indicates (www.researchgate.net). Allow a total mixing and reaction time of ~10–20 minutes. Use a clarifier detention of ~0.5–2.0 hours and a surface loading of ~0.1 m³/m²·h (360 m³/m²·d) or lower. Overall removal is >95% Zn and >99% TSS/turbidity (www.researchgate.net). Trials also showed >69% COD and >99% turbidity removal (www.researchgate.net).
Sources and context
The flow, concentration and removal figures above come from Indonesian industry studies, EPA guidance and galvanizing process surveys. The 2020 pilot study on ZnO waste cited here (www.researchgate.net) (www.researchgate.net) supports the treatment performance. The global zinc and water-use statistics (iwaponline.com) (iwaponline.com) set the operating context. These peer-reviewed and government sources match the design parameters to practical outcomes and regulatory limits.