WhatsApp

Membrane systems

Toray SWRO Membranes

Updated

Betaqua Mild Steel Media Filter is a reliable solution for water filtration systems in various industrial applications. With robust construction, this product is designed for high efficiency in.

Toray SWRO Membranes

Discuss the application.

Send the application, operating conditions and the result you expect. Our team will discuss the options with you.

Ask about this product

or use the contact page

PT Beta Pramesti Asia

Toray TM800V Series - Reverse Osmosis Membrane for Seawater Desalination

The Toray TM800V Series is a low-energy Reverse Osmosis (RO) membrane element specifically designed for desalination of seawater and high-salinity feedwater. The product utilizes advanced membrane technology that has gone through decades of research and development, and is manufactured with precision automation under ISO 9001 certification for quality consistency.

Product Advantages

  • Provides high quality permeate
  • Superior performance with up to 99.8% salt rejection
  • Robust chemical membrane for longer service life
  • High efficiency in treating high salinity water
  • Manufactured to consistent quality standards

Product Specifications

Product SpecificationsUnitTM810VTM820V-400TM820V-440
Size-404080408040
Membrane Areaft² (m²)87 (8)400 (37)440 (41)
Nominal Salt Rejection%99.899.899.8
Minimum Salt Rejection%99.5099.5099.50
Product Flow Rategpd (m³/d)1,900 (7.2)9,000 (34.1)9,900 (37.5)
Minimum Product Flow Rategpd (m³/d)1,550 (5.9)7,500 (28.4)8,250 (31.2)
Feed Spacer Thicknessmil283428

Operation Process

The TM800V Reverse Osmosis System works by passing feed water through a membrane to separate clean water (permeate) from salt concentrate (brine). Water enters the element through the feed line, then passes through the membrane, where clean water molecules separate from contaminants. Afterwards, the clean water comes out as permeate, while the remaining concentrate is discharged as brine.

Operational Specifications

ParameterMaximum Value
Maximum Operating Pressure (MPa)8.3
Maximum Feed Water Temperature (°C)45
Chlorine Concentration in Feedwater (ppm)Not detected
Operating pH Range2-11

Mode of Operation

The TM800V membrane utilizes the Reverse Osmosis process, where water is pressurized through a semi-permeable membrane to remove salts and other contaminants. The resulting clean water (permeate) is used for various purposes such as drinking and industrial water, while salts and other contaminants are discharged as brine.

Toray TM800M Series

Product Introduction

Toray TM820M-400 is a Reverse Osmosis (RO) membrane element with leading-edge technology designed for seawater desalination. It utilizes years of research and development and precision manufacturing processes to provide high permeate quality, improve performance, and extend membrane life. Ideal for high salinity seawater desalination applications, as well as industrial wastewater systems.

Key Benefits

  • High permeate quality with up to 99.8% salt rejection.
  • Has a longer membrane life thanks to the robust chemical composition of the membrane.
  • High efficiency in RO systems with high recovery.
  • Suitable for various applications such as seawater desalination and industrial wastewater.
  • Designed to operate at high pressure and temperature with stable performance.

Technical Specifications

SpecificationsTM820M-400TM820M-440
Membrane Area400 ft² (37 m²)440 ft² (41 m²)
Nominal Salt Rejection99.8%99.8%
Product Flow Rate7,000 gpd (26.5 m³/d)7,700 gpd (29.2 m³/d)
Feed Spacer Thickness34 mils28 mils

Product Working Process

The Toray TM820M-400 works on the principle of Reverse Osmosis, where feed water containing high salt is pressed through a semi-permeable membrane. This process separates clean water from salts and other particles, producing a high-quality permeate. Here are the main components involved in the system:

  • RO membrane: The main component that separates salts and impurities from water.
  • Pre-filter: Filters out large particles before the water enters the RO membrane.
  • High Pressure Pump: Ensures sufficient pressure to push the water through the membrane.
  • Control Valve: Regulates the flow and pressure of water in the system.

Operational Specifications

ParameterValues
Maximum Operating Pressure1,200 psi (8.3 MPa)
Maximum Feed Temperature113 °F (45°C)
Maximum SDI5
Feed Chlorine ConcentrationNot detected
Feed pH2-11

Want to Know More?

Contact us now for more information about the Toray TM800M-400 and how it can help improve the efficiency of your desalination system. Contact us now and get an attractive offer from us.