WhatsApp

Water and waste water chemical

Coagulant Water Treatment Indonesia

Updated

PAC and ACH coagulants from our own plant, certified SNI, Halal and NSF, plus POLYDADMAC, for WTPs and WWTPs. Select by jar test and plant trial.

Coagulant Water Treatment Indonesia

Discuss the application.

Send the application, operating conditions and the result you expect. Our team will discuss the options with you.

Ask about this product

or use the contact page

What is a coagulant in water treatment?

A coagulant is a chemical that neutralises the charge on fine particles, colloids and colour in water so they join into flocs that can be settled, floated by DAF, or filtered. The most widely used coagulants are PAC and ACH (aluminium-based) and the organic coagulant POLYDADMAC. PT Beta Pramesti Asia makes PAC and ACH in its own plant and supplies BETAGARD coagulants for water and wastewater treatment plants in Indonesia.

Updated: 12 November 2026.

Our plant has a capacity of 40,000 tonnes of PAC 12 per year and 12,000 tonnes of ACH per year, and our PAC and ACH are certified SNI, Halal and NSF. Plant, supply-form and quality-document details are on the PAC and ACH plant page.

Coagulant typeChemistryActive-content classWhen it is chosen
Liquid PACPoly aluminium chloride, medium basicityAbout 8–17% Al₂O₃Clarification of raw water, process water and wastewater with continuous dosing
Powder PACPoly aluminium chlorideAbout 28–30% Al₂O₃Compact storage with on-site dissolving
ACHAluminium chlorohydrate, high basicity22–24% Al₂O₃Low-alkalinity water or where the pH change must stay small
POLYDADMACCationic organic polymerNo Al₂O₃Coagulant aid or primary coagulant for DAF, filtration and dewatering

A coagulation programme is usually paired with flocculants, sludge treatment, or broader water and waste water chemicals. Chemical name and active content help screen candidates, but the dose is still set by a jar test on an actual sample and confirmed in a plant trial. Compare the types on the PAC and ACH pages and in the PAC versus alum comparison.

Before selecting a product, use the chemical wastewater treatment method guide to map contaminants, process sequence, jar-test gates, residuals, and sludge consequences.

PAC, ACH, or POLYDADMAC coagulants: when are they used?

Operator questionField conditionRelevant product or programData to check
Which supplier provides coagulants and flocculants for industrial wastewater in Indonesia?TSS, turbidity, color, or oil is not dropping in a clarifier, DAF, or sedimentation processThe Betagard series on this page and flocculantspH, alkalinity, turbidity, TSS, color, oil and grease, flow rate, and jar-test results
When should PAC be selected for raw water or process water?An inorganic coagulant is needed for surface water, process water, or wastewater clarificationBETAGARD 4008, 4010, 4012, 4017, 4031, 4033, and PACInitial pH, PAC dosage, aluminum residual, turbidity before and after treatment, and floc formation
When should ACH or aluminum chlorohydrate coagulants be considered?The process needs a high-Al2O3 coagulant or coagulant aid for liquid-solid separationBETAGARD 4040, 4040 Series, 4041, 4044, and 4045Jar-test result, operating pH, sludge character, color, organic matter, and material compatibility
When is an organic POLYDADMAC coagulant used?The system needs a primary coagulant or coagulant aid for clarification, DAF, filtration, centrifugation, or dewateringBETAGARD 4050 and 4050 SeriesTSS, color, oil and grease, separation unit type, sludge dry solids, and injection point

For chemical injection equipment, see Beta dosing pumps or Watermart dosing pumps for water treatment. If the plant’s baseline coagulant is alum, use the PAC-versus-alum comparison to align test basis, pH, alkalinity, sludge, and programme cost before requesting a quotation.

RFQ data that determines a wastewater coagulant trial

A wastewater coagulant RFQ should define influent character, the separation unit, current chemistry, effluent targets, and sludge-handling limits. Those facts determine the candidates and test design; where the requirement is already specific to polyaluminium chloride, use the PAC coagulant supplier page to compare grades, packaging, and supply-price basis.

RFQ dataDetails to recordDecision affected
Wastewater profileWaste source, continuous or batch operation, average/peak flow, pH, alkalinity, TSS, colour, oil and greaseSample type, test range, pH correction, and chemical candidates
Current chemical programmeProduct name, actual dose, solution concentration, injection order and pointComparison baseline and whether a chemical should be replaced or paired
Separation unitClarifier, sedimentation, DAF, filtration, centrifugation, or dewateringRequired floc-formation speed, floc strength, and separation time
Dosing systemTank capacity and material, mixer, pump, calibration result, and interlocksAbility to handle the product form and maintain the true dose
Target and sludge routeEffluent target, sludge volume, withdrawal frequency, and dewatering responseTrial limits that avoid transferring the problem to sludge handling
Supply requirementMonthly consumption, packaging, site location, unloading access, and safety stockQuotation basis and supply schedule after a candidate passes the trial

Coagulant jar-test acceptance table

A coagulant jar test is useful for quotation only when candidates are compared on the same sample, pH, mixing time, separation time, and quality target. Record the result as programme cost per m³ or per kg of TSS removed, not only as mg/L of product.

Test evidenceHow to normalize itDecision boundary
Product dosemg/L as supplied, solution concentration, and active content where availablePrevents liquid PAC, PAC powder, ACH, and POLYDADMAC from being compared on different bases
Water conditionInitial/final pH, alkalinity, TSS, colour, oil and grease, and temperatureShows whether performance comes from coagulation or only pH correction
Floc formationFloc speed, size, strength, and shear responseSelects a product that survives the actual mixer, pump, DAF, or clarifier
Treated-water qualityTurbidity, TSS, colour, oil and grease, COD where relevant, and metal residualConnects the bench test to effluent or process-water targets
Sludge impactSludge volume, settleability, cake/filtrate if tested, and flocculant needAvoids a choice that transfers cost to dewatering
Programme costProduct, pH correction, polymer, sludge handling, and supply frequencyDefines the real cost after all supporting chemicals are counted

To compare liquid PAC, PAC powder, ACH, and POLYDADMAC fairly, create two dose numbers: as-supplied product dose and active or Al2O3 basis where data are available. This matters because a product with a higher price per kg can still cost less when active content, pH correction, or sludge impact is better.

Dose normalizationPractical formulaWhen to use it
As-supplied productmg/L of product added to the sampleDaily consumption, stock, and delivered-price basis
Active or Al2O3 basismg/L product × active percentageComparing PAC/ACH grades without treating dilution water as active material
Cost per m³dose mg/L × flow m³/day × price/kg ÷ 1,000Estimating chemical cost at the same flow
Complete programme costcoagulant + pH adjustment + flocculant + sludge handlingSelecting the programme with the true lower operating cost

If two candidates reach the same effluent quality, choose the one that remains stable on normal and peak-load samples, not the one that looks clearest in a single beaker. For DAF or sludge applications, continue testing with sludge treatment so underflow, cake, and filtrate are included.

How should a jar-test result move to a plant trial?

A jar-test result should move to a plant trial only when dose, pH, injection sequence, and quality targets are written down. PT Beta Pramesti Asia usually asks for an operating baseline before the trial so a coagulant change is not confused with a change in flow, pH, TSS load, oil, or clarifier and DAF condition.

Requirement before trialMinimum evidenceWhy it matters
Sample represents operationSampling time, flow, pH, TSS, colour, oil and grease, and production conditionAvoids choosing a product from a sample that is too light or too severe
Dose can be injectedSolution concentration, pump capacity, injection point, and mixing timeConfirms the test dose is actually delivered in the plant
Quality target is clearTurbidity, TSS, colour, FOG, COD where relevant, and sludge limitsDefines when the trial is accepted or stopped
Sludge impact is countedSludge volume, settleability, polymer demand, cake, and filtratePrevents cost from moving from treated water to dewatering

Betagard Coagulant Series

BETAGARD 4008

Polyaluminum Chloride

BETAGARD 4008 is a yellow to amber colored liquid, functioning as a coagulant aid or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4008 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%BasicityDosage & Usage InstructionsHandling PrecautionsPackaging
Clear to yellowish liquid.Min 8%Min 1.163,0 - 5.0Min. 35%The actual dosage for BETAGARD 4008 should be determined in a tube test in the laboratory. Please ask your technical assistant for tube tests or plant trials.BETAGARD 4008 is a mildly acidic, stable under ordinary conditions substance. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics and other more resistant materials. Galvanized equipment should not be used. Tightly seal drum containers after use. See MSDS for additional information.Available in 25, 30 KG per bucket, 220 KG per plastic drum or 1200 KG per tote.

BETAGARD 4010

Polyaluminum Chloride 10%

BETAGARD 4010 is a clear to yellowish liquid, functioning as a coagulant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4010 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%BasicityDosage & Usage InstructionsHandling PrecautionsPackaging
Clear to yellowish liquid.Min 10%Min 1.193,0 - 5.0Min. 35%The actual dosage for BETAGARD 4010 should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4010 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. Refer to MSDS for additional information.Available in 25, 35 KG per bucket, 240 KG per plastic drum or 1200 KG per tote.

BETAGARD 4012

POLYALUMUNIUM CHLORIDE 12%

BETAGARD 4012 is a yellow to dark amber colored liquid, functioning as a coagulant aid or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4012 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by a surface electrostatic charge that prevents the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%BasicityDosage & Usage InstructionsHandling PrecautionsPackaging
Clear to yellowish liquid.Min 12%Min 1.243,0 - 5.0Min. 35%The actual dosage for BETAGARD 4012 should be determined in a tube test in the laboratory. Please ask your technical assistant for tube tests or plant trials.BETAGARD 4012 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. See MSDS for additional informationAvailable in 25, 35 KG per bucket, 240 KG per plastic drum or 1200 KG per tote.

BETAGARD 4012 Series

RAW WATER CLARIFIER COAGULANT AID POLYALUMUNIUM CHLORIDE (PAC)

BETAGARD 4012 Series is a yellow to dark amber colored liquid, functioning as a coagulant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4012 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%BasicityDosage & Usage InstructionsHandling PrecautionsPackaging
Yellowish to brown liquid.Min 12%1.19 - 1.403,5 - 5.0Min. 45%The actual dosage for BETAGARD 4012 Series should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4012 Series is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly seal drum containers after use. Refer to MSDS for additional information.Available in 200 Liter or 1000 Liter sizes.

BETAGARD 4017

POLYALUMUNIUM CHLORIDE 17%

BETAGARD 4017 is a clear to yellowish liquid, functioning as an auxiliary coagulant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4017 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%BasicityDosage & Usage InstructionsHandling PrecautionsPackaging
Clear to yellowish liquid.Min 17%Min 1.303,0 - 5.0Min. 35%The actual dosage for BETAGARD 4017 should be determined in a tube test in the laboratory. Please ask your technical assistant for tube tests or plant trials.BETAGARD 4017 is a mildly acidic, stable under ordinary conditions substance. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics and other more resistant materials. Galvanized equipment should not be used. Tightly seal drum containers after use. See SDS for additional information.Available in 25, 35 KG per bucket, 240 KG per plastic drum or 1300 KG per tote.

BETAGARD 4031

PAC POWDER

BETAGARD 4031 is a white powder, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. BETAGARD 4031 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203pH 1%InsolubleDosage & Usage InstructionsHandling PrecautionsPackaging
White powder.Min 30%3,5 - 5.0Max. 0.05%The actual dosage for BETAGARD 4031 should be determined in a tube test in the laboratory. Please ask your technical assistant for tube tests or plant trials.BETAGARD 4031 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. See SDS for additional information.Available in 25 Kg/bag.

BETAGARD 4033

PAC POWDER

BETAGARD 4033 is a yellow colored powder, functioning as a coagulant adjuvant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4033 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203pH 1%InsolubleDosage & Usage InstructionsHandling PrecautionsPackaging
Yellow colored powder.Min 28%3,5 - 5.0Max. 1,5%The actual dosage for BETAGARD 4033 should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4033 is moderately acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. See SDS for additional information.Available in 25 Kg/bag.

BETAGARD 4040

ALUMINUM CHLOROHYDRATE (ACH)

BETAGARD 4040 is a clear colorless liquid with a high Al2O3 content, functioning as a coagulant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4040 is specifically used in water and wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
Clear to slightly hazy colored liquid.22 - 24%1.33 - 1.38 @ 20°C3,0 - 5.0Actual dosage should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4040 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. Refer to MSDS for additional information.Available in 30 Kg, 270 Kg or 1350 Kg plastic container sizes.

BETAGARD 4040 Series

RAW WATER COAGULANT AID ALUMINUM CHLOROHYDRATE (ACH)

BETAGARD 4040 Series is a clear colorless liquid with a high Al2O3 content, functioning as a coagulant aid or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4040 is specifically used in water and wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
Clear to slightly hazy colored liquid.22 - 24%1.30 - 1.38 @ 20°C3,0 - 5.0Actual dosage should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4040 Series is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly seal drum containers after use. See MSDS for additional information.Available in plastic container sizes of 200 Liters/drum or 1000 Liters/IBC tank.

BETAGARD 4041

ALUMINUM CHLOROHYDRATE+

BETAGARD 4041 is a technically advanced high performance coagulant based on aluminum chlorohydrate blended with organic polymers, scientifically formulated for the treatment of industrial effluents including wastewater from food and dairy processing; and the oil, textile and chemical industries. BETAGARD 4041 is a clear yellow to amber colored liquid with high Al2O3 content, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. BETAGARD 4041 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
Clear to slightly hazy colored liquid.Min. 23%1.32 - 1.38 @ 20°C3,5 - 5.0Actual dosage should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4041 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly seal drum containers after use. See MSDS for additional information.Available in 30, 300 and 1300 kgs plastic container sizes.

BETAGARD 4044

ALUMINUM CHLOROHYDRATE+

BETAGARD 4044 is a technically advanced high performance coagulant based on aluminum chlorohydrate blended with organic polymers, scientifically formulated for the treatment of industrial effluents including effluents from food and dairy processing; and the oil, textile and chemical industries. BETAGARD 4044 is a clear colorless liquid with a high Al2O3 content, functioning as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. BETAGARD 4044 is specifically used in water & wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 10%Dosage & Usage InstructionsHandling PrecautionsPackaging
Yellow to amber colored liquid.15%1.20 - 1.30 @ 20°C3,0 - 5.0The actual dosage should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4044 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. See MSDS for additional information.Available in plastic container sizes with net weights of 30, 300, and 1300 kg.

BETAGARD 4045

ALUMINUM CHLOROHYDRATE (ACH)

BETAGARD 4045 is a clear colorless liquid with a high Al2O3 content, functioning as a coagulant or sludge conditioning agent in the liquid-solids separation process. BETAGARD 4045 is specifically used in water and wastewater treatment to reduce suspended solids (tubidity), color and other contaminants such as natural organic matter from surface water, colloidal particles, salts and clays stabilized by surface electrostatic charges that prevent the particles from coalescing.

Technical Specifications

Physical Form%Al203Specific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
Clear to slightly hazy colored liquid.22 - 24%1.33 - 1.38 @ 20°C3,5 - 5.0Actual dosage should be determined in a tube test in the laboratory. Please ask your technical assistant for jar tests or plant trials.BETAGARD 4045 is moderately acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. Refer to MSDS for additional information.Available in 30 kg, 270 kg or 1350 kg plastic container sizes.

BETAGARD 4050

ORGANIC COAGULANT

BETAGARD 4050 is a concentrated liquid of low molecular weight, cationic polydiallyl dimethyl ammonium chloride or POLYDADMAC which functions effectively as primary coagulant or coagulant aid in water or wastewater clarification. It is chlorine-resistant and effective over a wide pH range, and can substitute or be used in conjunction with inorganic primary coagulants such as alum and ferric salts. The maximum recommended concentration of BETAGARD 4050 in the treatment of potable water is 20 ppm. BETAGARD 4050 is also recommended for other liquid-solids separation processes, such as :

  • Dewatering of a wide range of industrial and municipal sludge;
  • Removal of suspended solids from wastewater;
  • Gravity settling;
  • Filtration;
  • Centrifugation;
  • Air flotation;
  • Oil and water separation;
  • Color Removal.

Technical Specifications

Physical FormSpecific gravityIonic ChargeHandling PrecautionsPackaging
Colorless to yellow clear liquid.1.33 - 1.38 @ 20°CVery HighBETAGARD 4050 is moderately corrosive to aluminum, iron and copper, including their alloys. Storage and feeding equipment should be made of plastic or FRP. To maintain polymer activity, storage temperature should not be higher than 38°C. Spills of BETAGARD 4050 can be easily rinsed off with plenty of water.Available in plastic container sizes with a net weight of 30 kg, 200 kg or 1000 kg.

Dosage & Application Instructions:

Clarification: 1 - 30 ppm Floatation: Up to 20 ppm Sludge Dewatering: 5 - 40 kg per ton of dry solids.

Actual dosage should be determined in laboratory tube tests. For best performance results, BETAGARD 4050 should be diluted with clean water and metered continuously to the system using a corrosion resistant positive displacement pump.

BETAGARD 4050 Series

Raw Water Clarifier Floculant

BETAGARD 4050 Series is a low molecular weight concentrated liquid, cationic polydiall dimethyl ammonium chloride or POLYDADMAC that functions effectively as a primary coagulant or coagulant aid in water or wastewater clarification. This product is chlorine resistant and effective over a wide pH range, and can replace or be used in conjunction with inorganic primary coagulants such as alum and ferric salts. The maximum recommended concentration for BETAGARD 4050 in drinking water treatment is 20 ppm. BETAGARD 4050 is also recommended for other liquid-solids separation processes, such as:

  • Dewatering of various industrial and municipal sludges;
  • Removal of suspended solids from wastewater;
  • Gravity settling;
  • Filtration;
  • Centrifugation;
  • Air floatation;
  • Separation of oil and water;
  • Color Removal.

Technical Specifications

Physical FormSpecific gravityIonic ChargeHandling PrecautionsPackaging
Clear to yellowish colored liquid.1.00 - 1.25 @ 20°CVery HighBETAGARD 4050 is moderately corrosive to aluminum, iron and copper, including their alloys. Storage and feeding equipment should be made of plastic or FRP. To maintain polymer activity, storage temperature should not be higher than 38°C. Spills of BETAGARD 4050 can be easily rinsed off with plenty of water.Available in plastic container sizes with a net weight of 200 Liters/drum.

Dosage & Usage Instructions:

Clarification: 1 - 30 ppm Floatation: Up to 20 ppm Sludge Dewatering: 5 - 40 kg per ton of dry solids.

Actual dosage should be determined in laboratory tube tests. For best performance results, BETAGARD 4050 should be diluted with clean water and metered continuously to the system using a corrosion resistant positive displacement pump.

FAQ

Who supplies coagulants and flocculants for wastewater treatment in Indonesia?

PT Beta Pramesti Asia makes PAC and ACH in its own plant (40,000 tonnes of PAC 12 and 12,000 tonnes of ACH per year) and supplies Betagard coagulants in Indonesia for water clarification, wastewater treatment, DAF, oil-water separation, and sludge conditioning. Where stronger floc formation is needed, the coagulant program can be paired with flocculants.

What is the difference between PAC, ACH, and organic coagulants?

PAC on this page includes polyaluminum chloride products such as BETAGARD 4008, 4010, 4012, 4017, 4031, and 4033. ACH includes aluminum chlorohydrate products such as BETAGARD 4040, 4041, 4044, and 4045. Organic coagulants such as BETAGARD 4050 are based on POLYDADMAC and are used as a primary coagulant or coagulant aid for clarification, DAF, filtration, centrifugation, and dewatering.

Can coagulant dosage be selected directly from the product table?

No. The product tables help identify physical form, pH, active content, and packaging, but the actual dosage should be determined through a tube test or jar test in the laboratory and confirmed through a plant trial. pH, alkalinity, turbidity, TSS, color, oil and grease, flow rate, and sludge characteristics should be prepared before a dosage recommendation is made.

When should a plant contact Beta for a coagulation program review?

Contact Beta when clarification, DAF, filtration, or sedimentation is unstable; turbidity, TSS, colour, or oil remains high; flocs break; chemical use rises; or sludge is difficult to separate. Send the system data through Beta’s contact page so the product options and field-trial requirements can be reviewed.

Jar-Test Protocol for Coagulant Selection

A comparable jar test uses an actual sample, recorded initial pH, a fixed injection sequence, and the same mixing and settling times for every dose. The objective is not simply the lowest dose: it is the combination that produces stable treated water, separable floc and a sludge volume the downstream process can manage.

Test stepConditions to recordDecision criterion
Sample characterisationpH, alkalinity, turbidity, TSS, colour, oil/grease and temperatureEstablish whether PAC, ACH or an organic coagulant should be compared.
Rapid coagulationDose in each beaker, chemical order and mixing timeReject doses that create fragile floc, move pH outside the process range or need impractical aid levels.
Flocculation and separationSlow-mix time, settling or flotation time and supernatant clarityCompare the outcome with the downstream clarifier, DAF, filtration or dewatering step.
Residual verificationFinal pH, turbidity/TSS, colour and sludge characterSelect candidates that meet the facility’s effluent target and its operational and sludge-management limits.
Field trialFlow, injection point, actual dose and before/after trendConfirm performance at normal and peak loading before changing the routine programme.

Betagard coagulants can be paired with flocculants and a chemical dosing pump. Send the jar-test results, flow data and effluent target through Beta’s contact page so the recommendation can be checked against the actual process train.

Plant-Trial Decision Sheet for Coagulants

A jar-test candidate is not a routine programme until a plant trial proves water quality, unit operation, sludge impact and chemical use together. Establish a baseline before changing the programme, use an agreed dose window, and record feed conditions so results remain comparable across shifts.

Trial evidenceBaseline to recordRequirement for acceptance
Influent and effluent qualityFlow, pH, turbidity/TSS, colour, oil/grease and sample timeThe target is met on comparable samples, including the agreed loading conditions.
Chemical controlProduct, batch, solution concentration, pump setting/calibration and injection pointActual dose can be calculated and repeated; it does not rely on the pump-dial position alone.
Separation performanceFloc-formation time, settling/flotation, carryover and filter condition where relevantFloc survives to the separation unit without creating a new downstream upset.
Sludge impactVolume, withdrawal frequency, dry solids where measured and dewatering responseBetter water quality does not overload the sludge-handling route.
Operating stabilityShift results, alarms, upstream changes, rain or production batchThe dose window has response limits and an agreed fallback setting when feed quality changes.
Measured costkg or L/day at the same flow and loadCompare cost per water volume or pollutant mass treated, not package price alone.

Record the final decision as accepted, repeat required, or rejected, with the reason. Include the corresponding flocculant data when asking for review so the interaction between coagulation and floc formation is not assessed in isolation.

Technical reference: the U.S. EPA explains the roles of coagulation, flocculation, and jar testing in water treatment. Accessed 27 July 2026; wastewater-coagulant selection must still use the facility’s actual sample and process train.