WhatsApp

Article

Welding’s wet scrubbers trap metal-laden water. The fix is chemistry, not more water.

beta-pramesti-asiaindustry-automotiveprocess-welding

Air Scrubber in the Welding Area: pH, Metal Sludge, and Recycling That Cuts Waste

pH control, coagulation/flocculation and membrane filtration turn wet scrubber water from a "metal slurry" into process water that can be reused. They also cut clean water use and waste volume.

Welding fume is not just mist. It is a mixture of metal oxides and fine metals (Fe, Mn, Ni, Cr, Cu, Zn, etc.) from the base metal and the melting electrode. This includes potential Cr⁶⁺ in certain materials such as stainless or galvanized (CCOHS, welding fumes). In a [wet scrubber (spray or packed tower)](https://beta.co.id/blog/scrubber-asam-di-pabrik-galvanizing-kombinasi-venturi-packed-bed-mencetak-99-efisiensi), those particles are captured in the water. This forms a slurry, wash water loaded with TSS (total suspended solids) and dissolved metal ions.

Without treatment, turbidity and metal content stay high and the water is unfit for release into the environment. Environmental standards need facilities to precipitate metals, remove solids, and neutralize pH before the water is reused or discharged.

Composition of welding fume and implications for wet scrubbing

Welding fume on mild steel is mostly iron (Fe) with traces of Cr, Ni, Mn. On stainless or galvanized steel, Cr (including Cr⁶⁺/hexavalent chromium) and Zn become more dominant (CCOHS). As the fume accumulates, scrubber water becomes concentrated in TSS and can contain hazardous metal species in dissolved form. To reduce this load, we use pH control, coagulation/flocculation, clarification/filtration, and if needed membrane polishing.

pH control for metal precipitation

The first key is pH. Many metal ions only precipitate as hydroxides at a high enough pH. Industrial metal precipitation trains usually adjust pH to 8.5–10.0, with a common set point of ~9.0–9.2 to force the metals to form solids and settle out (STERC guide on metal precipitation). The minimum solubility points for metals such as Cu, Cd and Fe are in the 8.5–9.5 range (Cu ~9.0, Cd ~9.2, Fe ~9–10). Therefore a target of ~9 is usually chosen as a compromise.

However, scrubbing and coagulant addition can lower the pH. Hydrolyzed alum or FeCl₃ produces acid. One study noted, “TDS (total dissolved solids) and EC (electrical conductivity) values increased because of coagulant addition and the wastewater became acidic” (study in the Brazilian Journal of Chemical Engineering). Therefore, after coagulation there is usually a neutralization step. Alkali such as NaOH or lime is added to reach the target pH. Ideally the alkali is caustic soda, dosed precisely with a dosing pump to keep the process stable.

Important note: if the electrodes or materials contain chromium, any Cr⁶⁺ (hexavalent chromium) must first be reduced to Cr³⁺ (trivalent) before precipitation. This is common practice in metal precipitation circuits (STERC).

Coagulation/flocculation and solids removal

Once the pH is maintained, the metal hydroxide sludge and dust must be removed. The usual way is coagulation and flocculation, then clarification or filtration. Coagulants such as PAC and ACH, iron salts or polymers are mixed rapidly. Then the flocs grow in a flocculation tank for 15–30 minutes before they are separated. Industry practice is to precipitate the metals in an insoluble form, for example hydroxides, sulfides or carbonates, then remove them by conventional clarification. The sludge is then collected, thickened and dewatered for disposal.

In welding, the scrubber water carries metallic sludge. This sludge usually contains regulated metals such as Cd, Cr, Ni. Once it is thickened, it is usually classified as hazardous waste. The clear water (supernatant) can go back to the scrubber or be polished further. For this stage, facilities usually use PAC/ACH coagulants and add BETAGARD flocculant to make the floc stronger. Then they thicken the sludge with dewatering polymer before it goes to screw press dewatering.

A welding plant study recorded the actual performance. Turbidity fell from 690 NTU (nephelometric turbidity units/unit of turbidity) to 9.68 NTU, a 98.6% reduction. This was after coagulation with a 25% alum/75% FeCl₃ mixture at a dose of 2.5 g/L. Only this high dose was able to remove stubborn colloids (BJCE study). After coagulation, clarification using units such as a clarifier is the main separation path. In practice, TSS removal >95–99% is usually achieved.

Clarification and membrane filtration

After clarification, membranes can polish the remaining solids. A bench-scale tubular ultrafiltration (UF) system was reported to remove "almost all" precipitated solids and produce clear filtrate. In other industries, clean UF permeate can go directly to reverse osmosis or back to the process. Therefore integrating ultrafiltration is a strong polishing option.

In a trial at a welding electrode plant, post-clarification water was fed to nanofiltration. The permeate result was “excellent”. COD (chemical oxygen demand) fell below 2 mg/L, TDS rejection approached 82%, turbidity <1 NTU, and hardness <100 mg/L as CaCO₃. Therefore reuse of treated water is possible (BJCE study). Even without UF, water clarified by coagulation alone is already “well below 10 NTU” and its dissolved metal content is much reduced. For membrane schemes, nano-filtration is suitable as polishing. If needed, UF permeate can also be directed to reverse osmosis depending on the quality target.

Scrubber circuit recycling and water savings

With effective treatment, [scrubber water can be recycled](https://beta.co.id/blog/scrubber-hemat-air-di-galvanizing-resirkulasi-pintar-phkonduktivitas-otomatis-dan-makeup), so make-up water demand falls sharply. Water recycling lets industry use less fresh water and discharge less wastewater. Recycling treated scrubber water cuts both consumption and effluent load.

A single welding cell that keeps reusing the same water with little blowdown (purge to control dissolved salts) uses much less water than a once-through system. Each cycle still adds a contaminant load (TDS, minor leaks), so some purge is needed. However, even a high recycle rate already gives large savings. Bleed can drop from hundreds of liters per hour to tens of liters per hour (BJCE study).

Environmental compliance and Indonesian standards

In Indonesia, there is no specific “welding” regulation. However, the wastewater standard for the metal plating industry sets limits for pH, metals (Cu, Ni, Zn, Cr⁶⁺, Cd), and TSS. Therefore scrubber water must be adjusted to the neutral range of 6–9 before discharge. To meet these limits, the steps above are usually needed: precipitation and removal of >90% solids, filtration/clarification, and pH neutralization.

Internationally, discharge from fabrication/metalworking is also usually subject to heavy metal rules. Failure to reduce metals/solids easily triggers violations. Note that “turbidity” control alone can be misleading. Metal load can remain high even when the water looks clear (US EPA document). From a business perspective, investment in coagulation/flocculation and recycling equipment saves on water and disposal costs while avoiding regulatory sanctions. Also, clean operation maintains permits and public image.

Technical summary and results achieved

Data from a Brazilian study on welding electrode wastewater show that coagulation–flocculation plus a membrane step produces water with turbidity <1 NTU and COD ≪2 mg/L (BJCE study). This water is ready for internal reuse and recirculation. A prescribed pH of 8.5–10.0 (target ~9.0–9.2) optimizes precipitation of metals such as Cu, Ni, Zn, Fe (STERC). A real-world coagulation example using 25% alum/75% FeCl₃ at a dose of 2.5 g/L reduced turbidity by 98.6% (690 → 9.68 NTU) (BJCE study). Tubular UF can filter “almost all” precipitated solids. NF shows TDS rejection of ~82% with hardness <100 mg/L (as CaCO₃) in the permeate (BJCE study), which opens the way for reuse and reduced discharge. This chemical and membrane integration, supported by our UF and NF equipment, is a consistent recipe for reducing water consumption and effluent load.